MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ti15Mo5Zr3Al ß titanium alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 882 MPa128000 psisolution heat treatment at 840°C
 882 - 1177 MPa128000 - 170700 psias forged and aged (600°C)
 1099 MPa159400 psisolution heat treatment at 740°C + aged at 600°C
Tensile Strength, Yield 870 MPa126000 psi0.2%, solution heat treatment at 840°C
 870 - 1173 MPa126000 - 170100 psias forged and aged (600°C)
 1087 MPa157700 psi0.2%, solution heat treatment at 740°C + aged at 600°C
Elongation at Break 15.3 %15.3 %solution heat treatment at 740°C + aged at 600°C
 15 - 20 %15 - 20 %as forged and aged (600°C)
 20 %20 %solution heat treatment at 840°C
Reduction of Area 57.5 %57.5 %solution heat treatment at 740°C + aged at 600°C
 43 - 80 %43 - 80 %as forged and aged (600°C)
 83.2 %83.2 %solution heat treatment at 840°C
Modulus of Elasticity 75.0 GPa10900 ksiSolution heat treated at 840°C
 88.0 GPa12800 ksiSolution heat treated at 740°C
 113 GPa16400 ksiSolution heat treated at 740°C + aged at 600°C
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.8 %3.8 %
Molybdenum, Mo 15 %15 %
Titanium, Ti 76.2 %76.2 %
Zirconium, Zr 5.0 %5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ti12Mo5Zr5Sn ß titanium alloy
Ti30Ta ß titanium alloy
Ti30Nb ß titanium alloy
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) Solution Treated 850°C (1560°F)
Overview of materials for Alpha/Beta Titanium Alloy

MMEDIC26 / 12402

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.