An acidic powdered binder system used to formulate high strength, hydraulic-setting cements for electrical potting or molding applications. A powder blend is typically formulated by adding one part binder to four parts filler by weight. Water is then added in a ratio of 15-20 parts to 100 parts powder blend by weight. Curing occurs at room temperature or can be accelerated by heating at 200 °F for 1-2 hours. |