MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: This grade is highly recommended for paper coating or for fiber extrusion.

TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics and good high frequency electrical and valuable acoustic/ultrasonic properties. Applications include medical and laboratory apparatus, microwave components and cookware and electronic components.

Information provided by Goodfellow. TPX® is a trademark of Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.833 g/cc0.0301 lb/in³ASTM D1505
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 260 °C
100 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 4242ASTM D785
Tensile Strength 10.0 MPa1450 psiASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 0.820 GPa119 ksiASTM D638
Flexural Strength 21.0 MPa3050 psiASTM D790
Flexural Modulus 0.630 GPa91.4 ksiASTM D790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
Izod Impact, Unnotched (ISO) 127 kJ/m²60.4 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.12.1ASTM D150
Dielectric Strength 65.0 kV/mm1650 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C65.0 µin/in-°FASTM E831
Melting Point 223 °C433 °FDSC Peak; JIS K7121
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 147 °C297 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46ASTM D542
Haze 2.1 %2.1 %ASTM D1003
Transmission, Visible 93 %93 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow TPX® MX002O Polymethylpentene
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
Mitsui TPX® DX820 Methylpentene Copolymer
Metflex EM67 Natural Rubber
Techmer ES HiFill® TPX-HTN-01043 A

PGOODF223 / 135575

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.