MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Glyptal 8240 Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL ready to spray equipment enamels are specially formulated coatings to me USASI #49, #61, and #33 gray standards. These sprayable, fast-dry, gloss enamels assure long life finishes and provide excellent shelf-life stability.

APPLICATION

GLYPTAL equipment enamels are designed for application through spray systems for finishing motors and equipment in the motor repair industry. The coatings may also be used for finishing transformers, machines, panelboards, switchgear, and other electrical and industrial equipment where fast-dry finish is required.

SURFACE PREPARATION

Surface to be coated should be dry, clean, and free from dirt, wax, oils, and other contaminants. Remove grease and oils by washing with mineral spirits or naphtha. Allow to dry thoroughly.

APPLICATION METHODS

Glyptal equipment enamels are supplied at a ready-to-spray viscosity. No further reduction is required to use on air atomized or airless spray equipment.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.13 g/cc0.0361 - 0.0407 lb/in³
Solids Content 28.5 - 33.5 %28.5 - 33.5 %Volume
 43.5 - 50 %43.5 - 50 %Weight
Fineness 6.06.0Hegman
Thickness 25.4 - 38.1 microns1.00 - 1.50 milDry Film
 76.2 - 127 microns3.00 - 5.00 milWet Film
 
Thermal PropertiesMetricEnglishComments
Flash Point <= 26.7 °C<= 80.0 °F
 
Optical PropertiesMetricEnglishComments
Gloss >= 70 %>= 70 %60° Specular
 
Processing PropertiesMetricEnglishComments
Dry Time 0.333 hour0.333 hourAir Dry
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ASA Number33Gray
Coverage500 ft²/galat 1 mil dry
MethodSpray
Recoat30 min
Solvent SystemXylene
SubstrateMetal
Viscosity25-30 sec#2 Zahn
 25-30 secReduced; #2 Zahn

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reade Advanced Materials Petalite Powder (Li2O·Al2O3·8SiO2)
Glyptal 8328 Enamel
Glyptal 8239 Enamel
Aperam N42 Cold Rolled Strip
3M Controltac™ 8620 ES Conformable Graphic Film

PGLYPT922 / 209761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.