MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 4548 Phenolic, Granular, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is available in black and brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.690 g/cc0.0249 lb/in³ASTM D1895
Density 1.47 g/cc0.0531 lb/in³ASTM D792
Water Absorption 0.215 %0.215 %ASTM D570
Linear Mold Shrinkage 0.0052 cm/cm0.0052 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8787ASTM D785
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM D638
Elongation at Break 0.80 %0.80 %ASTM D638
Tensile Modulus 9.00 GPa1310 ksiASTM D638
Flexural Strength 98.0 MPa14200 psiASTM D790
Flexural Modulus 9.00 GPa1310 ksiASTM D790
Compressive Strength 208 MPa30200 psiASTM D695
Poissons Ratio 0.340.34ASTM D638
Shear Modulus 3.36 GPa487 ksiCalculated
Izod Impact, Notched 0.171 J/cm0.320 ft-lb/inASTM D256
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ASTM D256
Impact 104104J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.10e+11 ohm-cm7.10e+11 ohm-cmASTM D247
Dielectric Constant 5.35.3ASTM D150
Dielectric Strength 12.3 kV/mm312 kV/inShort Time; ASTM D149
Dissipation Factor 0.0560.056ASTM D150
Arc Resistance 144 sec144 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 µm/m-°C
@Temperature 40.0 - 130 °C
36.1 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.440 W/m-K
@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 204 °C399 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 189 °C372 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 27.3 %27.3 %ASTM D2863
Shrinkage 0.199 %0.199 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2369 Phenolic, Granular, Compression Molded
Plenco 2311 Phenolic, Granular, Transfer Molded
Plenco 2311 Phenolic, Granular, Injection Molded
Plenco 2308 Phenolic, Granular, Transfer Molded
AGY ZenTron® S-2 Generic S-Glass Fiber

PLEL93 / 50668

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.