MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon™ 8A X Granular PTFE Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Teflon™ PTFE 8A X is a free-flowing white powder composed of relatively large particles and ideal for isostatic molding. Its most unique features are improved mold ability at lower pressure and improved surface smoothness of finished parts. It offers an excellent combination of properties that are characteristic of Teflon™ fluoroplastic resins. Teflon™ PTFE 8A X is often preferred for molding thick sheets and is sometimes used for ram extrusion of rod and tubing with thicker cross-sections. Properly processed products made from neat Teflon™ PTFE 8A X provide the superior properties typical of fluoroplastic resins. Many end products are fabricated from moldings of Teflon™ PTFE 8A X, such as: Ball valve seats, Seals, Discs, Lab ware, Pipe linings, Valves, Valve plugs, Ducting, Expansion bellows, Piston rings. Thick molded sheets are stock shapes made from Teflon™ PTFE 8A X.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D4894
Bulk Density 0.680 g/cc0.0246 lb/in³ASTM D4894
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Particle Size 490 µm490 µmAverage; ASTM D4894
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 6550 - 65ASTM D2240
Tensile Strength 41.4 MPa
@Thickness 0.130 mm
6000 psi
@Thickness 0.00512 in
skived tape; ASTM D4894
Elongation at Break 330 %
@Thickness 0.130 mm
330 %
@Thickness 0.00512 in
skived tape; ASTM D4894
Flexural Modulus 0.496 GPa71.9 ksiASTM D790
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched 1.87 J/cm3.50 ft-lb/inASTM D256
Coefficient of Friction 0.050 - 0.100.050 - 0.10ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+18 ohm>= 1.00e+18 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 0.100 mm
457 kV/in
@Thickness 0.00394 in
ASTM D149
Dissipation Factor <= 0.00010
@Frequency 1e+6 Hz
<= 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 sec>= 300 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °FASTM D3418
 327 °C621 °FSecond Peak; ASTM D4591
 342 °C648 °FInitial Peak; ASTM D4591
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.040 %<= 0.040 %ASTM D4894
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Detergent Resistance (hours)24On grit blast aluminum
 264
 624On aluminum
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)192ASTM B117. 5% NaCl at 35 °C (95 °F). On aluminum.
 744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Thermal Instability Index7.6ASTM D4894
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8833 / 268760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.