MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borstar® HE6062 HDPE Black Jacketing Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketing applications (i.e. low shrink-back, excellent stress-crack resistance, good melt strength and a wide processing window.)

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³Base; ASTM D792
 0.958 g/cc0.0346 lb/in³Compound; ASTM D792
ESCR 10% Igepal® >= 2000 hour
@Temperature 50.0 °C
>= 2000 hour
@Temperature 122 °F
ASTM D1693/B
Absorption Coefficient >= 400>= 400In kilo; ASTM D3349
Carbon Black Loading 2.5 %2.5 %ASTM D1603
Melt Flow  0.50 g/10 min
@Load 2.16 kg
0.50 g/10 min
@Load 4.76 lb
ASTM D1238/E
 2.0 g/10 min
@Load 5.00 kg
2.0 g/10 min
@Load 11.0 lb
ASTM D1238/P
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength, Ultimate >= 25.0 MPa>= 3630 psiASTM D638
Elongation at Break >= 700 %>= 700 %ASTM D638
Flexural Modulus 0.850 GPa123 ksiASTM D790/1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength >= 19.7 kV/mm>= 500 kV/inAt 50 mils; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= 76.0 °C<= 169 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature >= 235 °C>= 455 °F
Front Barrel Temperature >= 180 °C>= 356 °F
Head Temperature >= 235 °C>= 455 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Overview of materials for High Density Polyethylene (HDPE), Extruded
BASF Ultradur® B 6550 LN PBT
BASF Ultradur® B 6550 L PBT

PBOREA127 / 27434

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.