System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Thermx® CG923 BK010 PCT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polycyclohexylenedimethylene Terephthalate (PCT)
;
Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
Material Notes:
Thermx® CG923 BK010 is a 20% glass fiber reinforced, flame retardant, black polycyclohexylenedimethylene terephthalate resin for injection molding.
Celenese acquired the Thermx product line from DuPont in 2010.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.58
g/cc
1.58
g/cc
ASTM D 792
Density
1.58
g/cc
0.0571
lb/in³
ISO 1183
Filler Content
20 %
20 %
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
84
84
ASTM D 785
Tensile Strength at Break
100
MPa
14500
psi
ISO 527
Tensile Strength, Ultimate
99.0
MPa
@Temperature 23.0 °C
14400
psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break
1.8 %
1.8 %
ISO 527
2.1 %
@Temperature 23.0 °C
2.1 %
@Temperature 73.4 °F
ASTM D 638
Tensile Modulus
8.00
GPa
@Temperature 23.0 °C
1160
ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength
140
MPa
20300
psi
ASTM D 790
145
MPa
21000
psi
ISO 178
Flexural Modulus
6.75
GPa
979
ksi
ASTM D 790
7.40
GPa
1070
ksi
ISO 178
Izod Impact, Notched
0.450
J/cm
@Temperature 23.0 °C
0.843
ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched
430
J/cm
@Temperature 23.0 °C
806
ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO)
5.00
kJ/m²
@Temperature 23.0 °C
2.38
ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched
3.00
J/cm²
@Temperature 23.0 °C
14.3
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.500
J/cm²
@Temperature 23.0 °C
2.38
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
ASTM D 257
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
ASTM D 257
Dielectric Constant
3.0
@Frequency 1000 Hz,
Temperature 23.0 °C
3.0
@Frequency 1000 Hz,
Temperature 73.4 °F
ASTM D 150
3.0
@Frequency 10000 Hz,
Temperature 23.0 °C
3.0
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D 150
3.0
@Frequency 100000 Hz,
Temperature 23.0 °C
3.0
@Frequency 100000 Hz,
Temperature 73.4 °F
ASTM D 150
3.0
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.0
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D 150
Dielectric Strength
20.7
kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
526
kV/in
@Thickness 0.126 in,
Temperature 73.4 °F
500 V/s, Short Time; ASTM D149
Dissipation Factor
0.0030
@Frequency 100000 Hz
0.0030
@Frequency 100000 Hz
ASTM D 150
0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
ASTM D 150
0.013
@Frequency 1000 Hz
0.013
@Frequency 1000 Hz
ASTM D 150
0.021
@Frequency 10000 Hz
0.021
@Frequency 10000 Hz
ASTM D 150
Thermal Properties
Metric
English
Comments
Melting Point
283
°C
541
°F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
272
°C
522
°F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
437
°F
ISO 75-1/-2
234
°C
453
°F
ASTM D 648
UL RTI, Electrical
150
°C
@Thickness 1.50 mm
302
°F
@Thickness 0.0591 in
UL 746B
150
°C
@Thickness 3.00 mm
302
°F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact
130
°C
@Thickness 1.50 mm
266
°F
@Thickness 0.0591 in
UL 746B
130
°C
@Thickness 3.00 mm
266
°F
@Thickness 0.118 in
UL 746B
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL94
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
Processing Properties
Metric
English
Comments
Melt Temperature
300
°C
572
°F
Optimum
295
-
310
°C
563
-
590
°F
Mold Temperature
100
°C
212
°F
Optimum
80.0
-
120
°C
176
-
248
°F
Drying Temperature
95.0
°C
203
°F
Dry Time
4
-
6
hour
4
-
6
hour
Dehumidified Dryer
Moisture Content
<= 0.030 %
<= 0.030 %
Descriptive Properties
Color
Black
Drying Recommended
Yes
Features
Electrical Properties, Good
Flame Retardant
Filler
Glass fiber reinforcement
Forms
Pellets
Generic
PCT
Part Marking Code
>PCT-GF20FR(17)<
ISO 11469
Polymer Family
Polyester
Polymer Type
PCT
Processing Method
Injection Molding
Product Category
Electrical Resins
Flame Retardant Resins
Glass Reinforced Resins
Region Available
Americas
Asia/Pacific
Europe
Resin Identification
PCT-GF20FR(17)
ISO 1043
Uses
Connectors
E/E Applications
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Thermx® CG023 NC010 PCT
Celanese Thermx® TE1001 BK010 PCT
Celanese Thermx® TE3002 BK010 PCT
Celanese Thermx® CG043 BK010T PCT
Celanese Thermx® CG033 BK010T PCT
PDTA7730 / 89689
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.