MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials HCJ-48 Boron Nitride (BN) Powder  (discontinued **)
Categories: Ceramic; Nitride

Material Notes: Grade HCJ-48 is a coarse (-20 mesh), hexagonal Boron Nitride (BN) powder with a mean particle size of 200-250µ. It exhibits the unique properties of BN in a form readily used in the production of many advanced materials. Grade HCJ-48 has high apparent density and large crystal size, which contributes to excellent thermal properties and flow characteristics. surface area which contribute to excellent thermal properties and flow characteristics.

Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs. For use in: Electrically insulating/thermally conductive fillers for heaters, polymer matrices, adhesives, pastes and potting compounds. Lubrication applications for extreme heat or cold, extreme pressure, vacuum environments or harsh chemical exposures. Refractories and refractory coatings. Mold/die release. Metal/ceramic and ceramic/matrix composites.

General Characteristics of Boron Nitride: Electrical Insulator, Low Dielectric Constant, Low Dielectric Loss, High Temperature Stability, Thermal Conductor, Lubricious, Inert, Non-Wetting.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.00 g/cc0.0361 lb/in³Tap density
Particle Size 225 µm225 µmMean particle size is 225 µm. Crystal size is 10 µm.
Specific Surface Area 2.0 m²/g2.0 m²/g
 
Descriptive Properties
ColorWhite
Crystal StructureHexagonal(Graphitic)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials HCV Boron Nitride (BN) Powder
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder
Momentive Performance Materials AC-6028 Boron Nitride (BN) Powder
Titanium Dioxide, TiO2, Anatase
Titanium Dioxide, Rutile

CADV24 / 416

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.