MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grilamid® 2D 25 W 20 HL X black 9992 Nylon 6/12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Heat Stabilizer; Plasticizer; UV Stabilizer

Features: Good Flexibility; Good Impact Resistance; Heat Stabilized; High Viscosity; Hydrolysis Resistant; Plasticized

Uses: Automotive Applications; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Hydraulic Applications; Industrial Applications; Pneumatic Applications; Profiles; Tubing; Wire & Cable Applications

Appearance: Black

Forms: Granules

Processing Method: Extrusion; Profile Extrusion

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption 0.90 %0.90 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 2.1 %2.1 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 30.0 MPa4350 psiISO 2039-1
Tensile Stress at Strain 25.0 MPa
@Strain 50 %
3630 psi
@Strain 50 %
ISO 527-2
Elongation at Break >= 50 %>= 50 %ISO 527-2
Tensile Modulus 0.380 GPa55.1 ksiISO 527-1
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.20 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Strength 37.0 kV/mm940 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60012
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM013 / 307372

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.