MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Arlon Electronic Materials 92ML High Performance Halogen-Free Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Thermally conductive, multilayerable laminate and prepreg circuit board material. Available in various resin content percentages.

Arlon 92ML ceramic filled thermally conductive multifunctional epoxy laminate and prepreg products provide thermal performance with increased thermal conductivity of 2 W/m-K for multilayer PWBs for applications requiring thermal management throughout the entire board volume.

  • Engineered for use with metal backing for producing Metal-Clad PCBs

Typical Applications:

  • High brightness LEDs
  • DC-DC power converters
  • Automotive electronics
  • Electronic designs with limited thermal management alternatives

Information provided by ARLON Electronic Materials.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³ASTM D792 Method A
Water Absorption 0.12 %0.12 %IPC TM-650 2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiIPC TM-650 2.4.18.3
Flexural Strength 180 MPa26100 psiIPC TM-650 2.4.4
Peel Strength 0.841 kN/m4.80 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
 0.877 kN/m5.00 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+15 ohm-cm1.20e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
 1.50e+15 ohm-cm1.50e+15 ohm-cmE24/125; IPC TM-650 2.5.17.1
Surface Resistance 2.80e+14 ohm2.80e+14 ohmC96/35/90; IPC TM-650 2.5.17.1
 4.40e+14 ohm4.40e+14 ohmE24/125; IPC TM-650 2.5.17.1
Dielectric Constant  4.9
@Frequency 1e+9 Hz
4.9
@Frequency 1e+9 Hz
IPC TM-650 2.5.5.9
 5.2
@Frequency 1e+6 Hz
5.2
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
Dielectric Strength >= 39.4 kV/mm>= 1000 kV/inIPC TM-650 2.5.6.2
Dielectric Breakdown >= 50000 V>= 50000 VIPC TM-650 2.5.6
Dissipation Factor 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
Arc Resistance >= 150 sec>= 150 secIPC TM-650 2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 - 20.0 µm/m-°C10.6 - 11.1 µin/in-°Fx ,y direction; IPC TM-650 2.4.41
CTE, linear, Transverse to Flow  22.0 µm/m-°C
@Temperature <=180 °C
12.2 µin/in-°F
@Temperature <=356 °F
z (< Tg); IPC TM-650 2.4.24
 175 µm/m-°C
@Temperature >=180 °C
97.2 µin/in-°F
@Temperature >=356 °F
z (> Tg); IPC TM-650 2.4.24
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°FZ-axis; ASTM E1461
 3.50 W/m-K24.3 BTU-in/hr-ft²-°FX/Y-axis; ASTM E1461
Glass Transition Temp, Tg 170 °C338 °FDSC; IPC TM-650 2.4.25
 180 °C356 °FTMA; IPC TM-650 2.4.24
Decomposition Temperature 340 °C644 °FOnset; IPC TM-650 2.3.41
 400 °C752 °F5 percent; IPC TM-650 2.3.41
Flammability, UL94 V-0V-0
 
Descriptive Properties
Dielectric Withstand Voltage (VDC)> 5000HiPot; IPC TM-650 2.5.7.2
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 15IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 5IPC TM-650 2.4.24.1
Z-Axis Expansion (%)1.8IPC TM-650 2.4.24 (50-260°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive
Arlon Electronic Materials 99ML Thermally Conductive Epoxy
VICTREX Pipes™ PEEK polymer
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP

PARLM9860 / 149013

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.