MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Abatron AboCast/AboCure 8501-5/8501-4 High Temperature Resistant Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced; Epoxy, High Temperature

Material Notes: Gray, high viscosity, structural/dielectric epoxy with high temperature resistance.

Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be used at temperatures up to 300°C. Casting and assembly of tools, patterns, models and structural components that must operate in extremely hot and corrosive environments.

Processing: 100/41 ratio (pbw). Cured 2 hours at 95°C + 24 hour post-cure at 260°C.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 30000 cP
@Temperature 25.0 °C
30000 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.586 - 0.795 W/m-K4.06 - 5.51 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 300 °C572 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 1200 min
@Temperature 25.0 °C
1200 min
@Temperature 77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Cotronics Duralco™ 4525 Electrically Resistant, Room Temperature Curing Epoxy
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Cotronics Duralco™ 4703 Adhesive and Tooling Compound

PABKW010 / 22051

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.