Polyvinyl Chloride Homopolymer having high molecular weight, is white and free-flowing resins produced by suspension polymerization process. The resin can easily blend with variety of additives to achieve desired qualities properties e.g. high strength, needed in many applications. The high K value PVC resin is developed to serve the application which high mechanical properties e.g. high strength, strength, high pressure are needed. Applications: High strength flexible sheet (matt cover, etc.), Flexible profile, high strength & abrasion resistance flexible product (automotive parts, hose, etc.), High strength and thermal stability wire & cable, wire harness , High elasticity product (loop sandal, gear knob, brush, etc.) Features: Excellent plasticizer absorption and dry up abilities. Excellent electrical properties. Excellent mechanical performance of finished products. Information provided by SCG. |