MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 - 0.960 g/cc0.0335 - 0.0347 lb/in³Average value: 0.942 g/cc Grade Count:54
Moisture Vapor Transmission 1.30 - 1.65 cc-mm/m²-24hr-atm3.30 - 4.19 cc-mil/100 in²-24hr-atmAverage value: 1.44 cc-mm/m²-24hr-atm Grade Count:7
Oxygen Transmission 185 - 264 cc-mm/m²-24hr-atm470 - 671 cc-mil/100 in²-24hr-atmAverage value: 215 cc-mm/m²-24hr-atm Grade Count:7
Viscosity  1.00e+6 - 2.00e+6 cP
@Temperature 190 - 190 °C
1.00e+6 - 2.00e+6 cP
@Temperature 374 - 374 °F
Average value: 1.24e+6 cP Grade Count:5
 1.00e+6 - 2.00e+6 cP
@Shear Rate 50.0 - 50.0 1/s
1.00e+6 - 2.00e+6 cP
@Shear Rate 50.0 - 50.0 1/s
Average value: 1.24e+6 cP Grade Count:5
Vinyl Acetate Content 6.00 - 33.0 %6.00 - 33.0 %Average value: 19.3 % Grade Count:28
Melt Flow 0.400 - 43.0 g/10 min0.400 - 43.0 g/10 minAverage value: 11.0 g/10 min Grade Count:55
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55.0 - 96.055.0 - 96.0Average value: 78.2 Grade Count:14
Hardness, Shore D 19.0 - 45.019.0 - 45.0Average value: 31.5 Grade Count:16
Tensile Strength, Ultimate 3.03 - 17.0 MPa440 - 2470 psiAverage value: 10.2 MPa Grade Count:17
Film Tensile Strength at Yield, MD 4.00 - 9.00 MPa580 - 1310 psiAverage value: 6.08 MPa Grade Count:5
Film Tensile Strength at Yield, TD 3.70 - 10.0 MPa537 - 1450 psiAverage value: 6.74 MPa Grade Count:5
Tensile Strength, Yield 5.24 - 6.31 MPa760 - 915 psiAverage value: 5.69 MPa Grade Count:3
Film Elongation at Break, MD 360 - 600 %360 - 600 %Average value: 505 % Grade Count:12
Film Elongation at Break, TD 500 - 653 %500 - 653 %Average value: 572 % Grade Count:12
Elongation at Break 122 - 800 %122 - 800 %Average value: 732 % Grade Count:18
Elongation at Yield 170 - 260 %170 - 260 %Average value: 203 % Grade Count:3
Flexural Modulus 0.0125 - 0.101 GPa1.82 - 14.6 ksiAverage value: 0.0460 GPa Grade Count:12
Secant Modulus, MD 0.0380 - 0.120 GPa5.51 - 17.4 ksiAverage value: 0.0698 GPa Grade Count:6
Secant Modulus, TD 0.0430 - 0.125 GPa6.24 - 18.1 ksiAverage value: 0.0708 GPa Grade Count:6
Instrumented Impact Total Energy 10.8 - 38.0 J8.00 - 28.0 ft-lbAverage value: 23.7 J Grade Count:11
Coefficient of Friction 0.150 - 3.900.150 - 3.90Average value: 0.926 Grade Count:9
Elmendorf Tear Strength, MD 3.70 - 4.21 g/micron94.0 - 107 g/milAverage value: 3.91 g/micron Grade Count:7
Elmendorf Tear Strength, TD 3.70 - 5.24 g/micron94.0 - 133 g/milAverage value: 4.36 g/micron Grade Count:4
Dart Drop Test 85.0 - 700 g0.187 - 1.54 lbAverage value: 290 g Grade Count:5
Film Tensile Strength at Break, MD 15.0 - 31.0 MPa2180 - 4500 psiAverage value: 24.0 MPa Grade Count:12
Film Tensile Strength at Break, TD 13.0 - 39.0 MPa1890 - 5660 psiAverage value: 23.9 MPa Grade Count:9
 
Thermal PropertiesMetricEnglishComments
Melting Point 37.0 - 104 °C98.6 - 219 °FAverage value: 75.5 °C Grade Count:50
Vicat Softening Point 40.0 - 81.0 °C104 - 178 °FAverage value: 58.9 °C Grade Count:45
Brittleness Temperature -85.0 - -77.0 °C-121 - -107 °FAverage value: -82.3 °C Grade Count:3
 
Optical PropertiesMetricEnglishComments
Haze 2.00 - 48.0 %2.00 - 48.0 %Average value: 10.9 % Grade Count:14
Gloss 22.0 - 109 %22.0 - 109 %Average value: 66.6 % Grade Count:14
Transmission, Visible 4.50 - 75.0 %4.50 - 75.0 %Average value: 36.8 % Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 235 °C320 - 455 °FAverage value: 221 °C Grade Count:9
Melt Temperature 125 - 232 °C257 - 450 °FAverage value: 190 °C Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate

O4102 / 78292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.