VESTAMID® DX9310 BK E70399 is a PA 612 extrusion compound developed for the production of tubing systems, for example multilayer tubes used as air brake lines. Besides optimized processing behavior and improved cold impact resistance VESTAMID® DX9310 BK E70399 offers, owing to a special modification, similar mechanical properties as VESTAMID® X7393 (PA 12 based compound typically used for monolayer air brake tubing). Due to these properties it is suited as middle layer in the multilayer tube 250.1, together with VESTAMID® X7393 as inner and outer layer. VESTAMID® DX9310 BK E70399 is supplied as cylindrical pellets ready for processing in moisture-proof bags. Information on design of MLT 250.1 is contained in the corresponding product information of this MLT. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Dry properties listed below Industrial Sector: Automotive and Mobility, Sustainable Sustainability: Sustainable electricity Processing: Injection molding, Extrusion Delivery form: Pellets, Granules Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels Electrical: Insulating Conformity: Automotive Additives: Lubricant, Unfilled Applications: Tube and hose Processing: Pipe/Tube extrusion Special Characteristics: High impact strength, Light-stabilized, U.V. stabilized, High heat resistant, High viscosity Features: Deep-drawing property Color: Black Additives: Plasticizer, Impact restistant, Light stabilizer, Heat stabilizerInformation provided by Evonik. |