MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: Information provided by DSM Engineering Plastics.

Former DSM Engineering Plastics product line is now with Envalior.

Key Words: Polyamide 46
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³(DAM); ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psiISO 527-1/-2
Elongation at Break 3.5 %3.5 %ISO 527-1/-2
Tensile Modulus 8.00 GPa1160 ksiISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.24 ft-lb/in²ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 ohm-cm1.00e+8 ohm-cmIEC 60093
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Comparative Tracking Index 325 V325 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 295 °C563 °F(DAM); ISO 11357-1/-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TE250F6 PA46-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
Envalior Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
Envalior Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Röchling SUSTAMID® 46 PA 46

PDSMA014 / 30949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.