MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® LVX-65H SST nat PA12-GF65
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following product profile:
  • Very high stiffness and strength
  • Excellent impact and notched impact strength
  • Very low moisture absorption
  • Suitable for often repeated steam sterilization
  • Very high dimensional stability
  • Easy processing, good flow, characteristics
  • High molding precision, low warpage
Grilamid LVX-65H SST natural is suitable for production of technical parts in applications such as:
  • Electronic devices
  • Automotive
  • Mechanical engineering
  • Safety components
  • Medical devices and instruments
  • Sports and Leisure goods

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³Dry; ISO 1183
Water Absorption 0.80 %0.80 %Sim. to ISO 62
Moisture Absorption 0.400 %0.400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 200 MPa29000 psiConditioned; ISO 2039-1
Tensile Strength at Break 185 MPa26800 psiConditioned; ISO 527-1/-2
 210 MPa30500 psiDry; ISO 527-1/-2
Elongation at Break 2.5 %2.5 %Dry; ISO 527-1/-2
 2.5 %2.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 17.0 GPa2470 ksiConditioned; ISO 527-1/-2
 19.0 GPa2760 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 43.0 kV/mm1090 kV/inDry; IEC 60243-1
 43.0 kV/mm1090 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °C320 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesImproved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2558 Polycarbonate
EMS-Grivory Grilamid® LVX-65H SST black 9288 PA12-GF65
Lotte Advanced Materials Starex® GR-4030 ABS, 30% Glass Filled
EMS-Grivory Grilamid® LV-65H SST black 9288 PA12-GF65

PGRH093 / 156802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.