MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Thermx® CGT33 PCT, 30% Specialty
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: Thermx« CGT33 is a 30% glass fiber reinforced and toughened polycyclohexylenedimethylene terephthalate for injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Moisture Absorption 0.150 %0.150 %23°C/50%RH; ISO 62
Water Absorption at Saturation 1.4 %1.4 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.8 %2.8 %5mm/min; ISO 527-2/1A
Tensile Modulus 8.40 GPa1220 ksi50mm/min; ISO 527-2/1A
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 7.60 GPa1100 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 48.0 µm/m-°C26.7 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
Melting Point 285 °C545 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-1, -2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
Melt Temperature 295 - 310 °C563 - 590 °F
Drying Temperature >= 95.0 °C>= 203 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Thermx® CGT33 BK010T PCT
Celanese Thermx® CGT33 NC010 PCT

PHCQ467 / 178922

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.