MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 1.8 - 2.4 %1.8 - 2.4 %ISO 62
Water Absorption at Saturation 6.0 - 7.0 %6.0 - 7.0 %ISO 62
Viscosity Measurement 145145Viscosity index; ISO 307
Linear Mold Shrinkage 0.014 - 0.018 cm/cm0.014 - 0.018 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 270 MPa39200 psiISO 2039-1
Tensile Strength at Break 210 MPa30500 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 11.0 GPa1600 ksiISO 527
Charpy Impact Unnotched 2.80 J/cm²13.3 ft-lb/in²DIN 53453
 2.50 J/cm²
@Temperature -40.0 °C
11.9 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cmIEC 93
Surface Resistance 1e+05 - 1.00e+6 ohm1e+05 - 1.00e+6 ohm
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 250
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 3146 DSC
Maximum Service Temperature, Air 115 °C239 °FContinuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
440A Martensitic Stainless Steel (UNS S44002)
Avient Edgetek® NL-20CF/000 Nylon 6/12, Carbon Fiber Reinforced
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber

PFRI005 / 38926

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.