MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, Glass Bead Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.800 - 1.75 g/cc0.0289 - 0.0632 lb/in³Average value: 1.36 g/cc Grade Count:143
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 22.2 % Grade Count:22
Water Absorption 0.0500 - 7.00 %0.0500 - 7.00 %Average value: 1.37 % Grade Count:49
Moisture Absorption at Equilibrium 0.250 - 4.40 %0.250 - 4.40 %Average value: 1.91 % Grade Count:32
Water Absorption at Saturation 5.10 - 9.45 %5.10 - 9.45 %Average value: 6.30 % Grade Count:10
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.130 Grade Count:8
Linear Mold Shrinkage 0.00150 - 0.0280 cm/cm0.00150 - 0.0280 in/inAverage value: 0.0119 cm/cm Grade Count:121
 0.0100 - 0.0100 cm/cm
@Temperature 80.0 - 80.0 °C
0.0100 - 0.0100 in/in
@Temperature 176 - 176 °F
Average value: 0.0100 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00300 - 0.0190 cm/cm0.00300 - 0.0190 in/inAverage value: 0.0113 cm/cm Grade Count:38
 0.0120 - 0.0120 cm/cm
@Temperature 80.0 - 80.0 °C
0.0120 - 0.0120 in/in
@Temperature 176 - 176 °F
Average value: 0.0120 cm/cm Grade Count:2
Melt Flow 1.00 - 15.0 g/10 min1.00 - 15.0 g/10 minAverage value: 3.50 g/10 min Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 98.0 - 12298.0 - 122Average value: 118 Grade Count:29
Tensile Strength, Ultimate 35.0 - 165 MPa5080 - 23900 psiAverage value: 78.6 MPa Grade Count:124
 25.0 - 55.0 MPa
@Temperature 60.0 - 150 °C
3630 - 7980 psi
@Temperature 140 - 302 °F
Average value: 38.4 MPa Grade Count:2
Tensile Strength, Yield 55.0 - 125 MPa7980 - 18200 psiAverage value: 87.2 MPa Grade Count:23
Elongation at Break 0.500 - 50.0 %0.500 - 50.0 %Average value: 5.39 % Grade Count:130
 15.0 - 45.0 %
@Temperature 60.0 - 150 °C
15.0 - 45.0 %
@Temperature 140 - 302 °F
Average value: 26.3 % Grade Count:1
Elongation at Yield 2.40 - 20.0 %2.40 - 20.0 %Average value: 7.28 % Grade Count:12
 10.0 - 16.0 %
@Temperature 60.0 - 150 °C
10.0 - 16.0 %
@Temperature 140 - 302 °F
Average value: 13.8 % Grade Count:1
Modulus of Elasticity 1.60 - 10.0 GPa232 - 1450 ksiAverage value: 4.52 GPa Grade Count:102
 0.640 - 2.20 GPa
@Temperature 60.0 - 150 °C
92.8 - 319 ksi
@Temperature 140 - 302 °F
Average value: 1.21 GPa Grade Count:1
Flexural Yield Strength 58.6 - 238 MPa8500 - 34500 psiAverage value: 129 MPa Grade Count:113
Flexural Modulus 1.10 - 10.3 GPa160 - 1500 ksiAverage value: 4.49 GPa Grade Count:122
 1.25 - 3.05 GPa
@Temperature 60.0 - 120 °C
181 - 442 ksi
@Temperature 140 - 248 °F
Average value: 1.97 GPa Grade Count:1
Compressive Yield Strength 31.0 - 68.9 MPa4500 - 10000 psiAverage value: 49.6 MPa Grade Count:8
Izod Impact, Notched 0.160 - 0.801 J/cm0.300 - 1.50 ft-lb/inAverage value: 0.410 J/cm Grade Count:68
 0.350 - 0.350 J/cm
@Temperature -40.0 - -20.0 °C
0.656 - 0.656 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 0.350 J/cm Grade Count:1
Izod Impact, Unnotched 1.01 - 6.41 J/cm1.90 - 12.0 ft-lb/inAverage value: 3.18 J/cm Grade Count:43
Izod Impact, Notched (ISO) 1.50 - 80.0 kJ/m²0.714 - 38.1 ft-lb/in²Average value: 8.49 kJ/m² Grade Count:37
 2.00 - 7.00 kJ/m²
@Temperature -40.0 - -30.0 °C
0.952 - 3.33 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 4.00 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) 23.1 - 21000 kJ/m²11.0 - 9990 ft-lb/in²Average value: 32.8 kJ/m² Grade Count:6
 18.0 - 50.0 kJ/m²
@Temperature -30.0 - -30.0 °C
8.57 - 23.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 31.0 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.00 J/cm² - NB4.76 ft-lb/in² - NBAverage value: 3.35 J/cm² Grade Count:45
 1.00 - 4.50 J/cm²
@Temperature -40.0 - -20.0 °C
4.76 - 21.4 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 2.78 J/cm² Grade Count:16
Charpy Impact, Notched 0.200 - 1.80 J/cm²0.952 - 8.57 ft-lb/in²Average value: 0.605 J/cm² Grade Count:51
 0.0800 - 0.800 J/cm²
@Temperature -40.0 - -20.0 °C
0.381 - 3.81 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.429 J/cm² Grade Count:18
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10000 - 1.00e+17 ohm-cm10000 - 1.00e+17 ohm-cmAverage value: 4.31e+15 ohm-cm Grade Count:82
Surface Resistance 1.00e+7 - 1.00e+15 ohm1.00e+7 - 1.00e+15 ohmAverage value: 1.32e+14 ohm Grade Count:41
Dielectric Constant 3.50 - 6.003.50 - 6.00Average value: 4.25 Grade Count:29
Dielectric Strength 11.0 - 80.0 kV/mm280 - 2030 kV/inAverage value: 28.1 kV/mm Grade Count:60
Dissipation Factor 0.0100 - 0.2000.0100 - 0.200Average value: 0.0493 Grade Count:22
Dielectric Loss Index 0.0150 - 0.1500.0150 - 0.150Average value: 0.0825 Grade Count:8
Comparative Tracking Index 300 - 600 V300 - 600 VAverage value: 483 V Grade Count:34
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 73.8 µm/m-°C11.0 - 41.0 µin/in-°FAverage value: 52.4 µm/m-°C Grade Count:34
 40.0 - 58.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
22.2 - 32.2 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 49.0 µm/m-°C Grade Count:2
 40.0 - 58.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
22.2 - 32.2 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 49.0 µm/m-°C Grade Count:2
Thermal Conductivity 0.259 - 0.389 W/m-K1.80 - 2.70 BTU-in/hr-ft²-°FAverage value: 0.322 W/m-K Grade Count:11
Melting Point 220 - 265 °C428 - 509 °FAverage value: 258 °C Grade Count:63
Maximum Service Temperature, Air 80.0 - 220 °C176 - 428 °FAverage value: 134 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 190 - 260 °C374 - 500 °FAverage value: 228 °C Grade Count:62
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 255 °C158 - 491 °FAverage value: 157 °C Grade Count:120
Vicat Softening Point 215 - 250 °C419 - 482 °FAverage value: 241 °C Grade Count:33
Flammability, UL94 HB - V-0HB - V-0Grade Count:96
Oxygen Index 26.0 - 33.0 %26.0 - 33.0 %Average value: 27.3 % Grade Count:10
Glow Wire Test 649 - 750 °C1200 - 1380 °FAverage value: 655 °C Grade Count:19
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 300 °C500 - 572 °FAverage value: 283 °C Grade Count:29
Nozzle Temperature 250 - 304 °C482 - 580 °FAverage value: 275 °C Grade Count:13
Melt Temperature 241 - 310 °C465 - 590 °FAverage value: 281 °C Grade Count:81
Mold Temperature 49.0 - 120 °C120 - 248 °FAverage value: 85.2 °C Grade Count:105
Drying Temperature 75.0 - 107 °C167 - 225 °FAverage value: 82.5 °C Grade Count:75
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.163 % Grade Count:46
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:12
Injection Pressure 4.96 - 138 MPa720 - 20000 psiAverage value: 92.2 MPa Grade Count:55

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 6, Glass Bead Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled

O2510 / 78009

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.