  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem IG58 HDPE Injection Molding Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and output (fast cycle). Its applications include: thin-wall articles, housewares, ice cream packaging, and food and general purpose containers. IG58 has been developed for injection molding under conditions comparable to high-density polyethylene with a similar melt flow index. Recommended temperature profile: 160 to 230ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ASTM-D792
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ASTM-D2240
Tensile Strength at Break 11.0 MPa1600 psiASTM-D638
Tensile Strength, Yield 24.0 MPa3480 psiASTM-D638
Flexural Modulus, 1% Secant 1190 MPa173000 psiASTM-D790
Izod Impact, Notched 0.280 J/cm0.525 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C160 °FASTM-D648
Vicat Softening Point 125 °C
@Load 1.02 kg
257 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Braskem HC7260LS-L HDPE Injection Molding Polyethylene
Bamberger Polymers Bapolene® 3295 Polyethylene, Injection Grade
Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding
Borealis Borstar® CB9600 HDPE for Extrusion Coating

PBRAS903 / 106749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.