MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1005 Steel
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: AISI 1005 Low Carbon Steel

Key Words: UNS G10050, AISI1005, ASTM A29, ASTM A510, MIL SPEC MIL-S-11310 (CS1005), SAE J403, SAE J412
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.872 g/cc0.2844 lb/in³Composition 0.06% C, 0.38% Mn, 0.01% Si, annealed at 925°C
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.6 µm/m-°C
@Temperature 0.000 - 100 °C
7.00 µin/in-°F
@Temperature 32.0 - 212 °F
 13.1 µm/m-°C
@Temperature 0.000 - 200 °C
7.28 µin/in-°F
@Temperature 32.0 - 392 °F
 13.5 µm/m-°C
@Temperature 0.000 - 300 °C
7.50 µin/in-°F
@Temperature 32.0 - 572 °F
 13.7 µm/m-°C
@Temperature 0.000 - 400 °C
7.61 µin/in-°F
@Temperature 32.0 - 752 °F
 13.7 µm/m-°C
@Temperature 0.000 - 1000 °C
7.61 µin/in-°F
@Temperature 32.0 - 1830 °F
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
7.89 µin/in-°F
@Temperature 32.0 - 932 °F
 14.6 µm/m-°C
@Temperature 0.000 - 600 °C
8.11 µin/in-°F
@Temperature 32.0 - 1110 °F
 14.9 µm/m-°C
@Temperature 0.000 - 700 °C
8.28 µin/in-°F
@Temperature 32.0 - 1290 °F
 16.6 µm/m-°C
@Temperature 0.000 - 800 °C
9.22 µin/in-°F
@Temperature 32.0 - 1470 °F
Specific Heat Capacity  0.481 J/g-°C
@Temperature >=100 °C
0.115 BTU/lb-°F
@Temperature >=212 °F
 0.519 J/g-°C
@Temperature 150 - 200 °C
0.124 BTU/lb-°F
@Temperature 302 - 392 °F
 0.536 J/g-°C
@Temperature 200 - 250 °C
0.128 BTU/lb-°F
@Temperature 392 - 482 °F
 0.553 J/g-°C
@Temperature 250 - 300 °C
0.132 BTU/lb-°F
@Temperature 482 - 572 °F
 0.595 J/g-°C
@Temperature 350 - 400 °C
0.142 BTU/lb-°F
@Temperature 662 - 752 °F
 0.662 J/g-°C
@Temperature 450 - 500 °C
0.158 BTU/lb-°F
@Temperature 842 - 932 °F
 0.754 J/g-°C
@Temperature 550 - 600 °C
0.180 BTU/lb-°F
@Temperature 1020 - 1110 °F
 0.846 J/g-°C
@Temperature 850 - 900 °C
0.202 BTU/lb-°F
@Temperature 1560 - 1650 °F
 0.867 J/g-°C
@Temperature 650 - 700 °C
0.207 BTU/lb-°F
@Temperature 1200 - 1290 °F
 1.105 J/g-°C
@Temperature 700 - 750 °C
0.2641 BTU/lb-°F
@Temperature 1290 - 1380 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Iron, Fe 99.5 - 100 %99.5 - 100 %As remainder
Manganese, Mn <= 0.35 %<= 0.35 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1006 Steel, cold drawn
AISI 1009 Steel
Overview of materials for Low Carbon Steel
AISI 1010 Steel, cold drawn
AISI 1006 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round

M1005A / 6773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.