MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Fiber Filled

Material Notes: Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance and machinability which account for its widespread use on electrical, telecommunication and appliance applications.

Durez 152 is fungus resistant per Mil-I-631D and Mil-E-5272C

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.5 g/cc0.054 lb/in³ASTM D792
Apparent Bulk Density 0.68 g/cc0.025 lb/in³ASTM D1895
Water Absorption 0.3 %0.3 %ASTM D570
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 48 MPa7000 psiASTM D638
Tensile Modulus 9.6 GPa1400 ksiASTM D638
Flexural Strength 76 MPa11000 psi
Compressive Strength 207 MPa30000 psiASTM D695
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.8 kV/mm325 kV/inStep by step; ASTM D149
 14.7 kV/mm373 kV/inShort Time; ASTM D149
Dissipation Factor 0.050
@Frequency 1e+6 Hz
0.050
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 190 V190 VIEC Tracking Index
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °FUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 191 °C376 °FASTM D648
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade
Plywood
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade

P90X09a / 142664

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.