MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Description

CP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact strength, excellent stress crack resistance, and good gloss.
Application

CP 808-01 meets the specification contained in FDA Regulation 21CFR177.1520(c)3.1.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.924 g/cc0.924 g/ccASTM D792
ESCR 100% Igepal® 250 hour250 hourCondition C; ASTM D1693
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength, Yield 11.0 MPa1600 psi2"/min; ASTM D638
Elongation at Break 175 %175 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 317 MPa46000 psiASTM D790
Falling Dart Impact 28.5 J
@Temperature -40.0 °C
21.0 ft-lb
@Temperature -40.0 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -68.0 °C-90.4 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 122 °C252 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
A. Schulman CP814-01 Linear, Low-Density Polyethylene
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade

PASHU070 / 25034

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.