MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phosphorus (III) Bromide, PBr3
Categories: Ceramic; Halide; Fluid; Solvent

Material Notes: CAS Number: 7789-60-8

Physical Form: Colorless Liquid

Key Words: PBr3, Phosphorous, Phosphorus Bromide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³
Molecular Weight 270.686 g/mol270.686 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Temperature 438 °C820 °F
Critical Molar Volume 300 cm³/mol18.3 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 143.3 J/g61.66 BTU/lbAt Boiling Point
Specific Heat Capacity 0.2808 J/g-°C0.06711 BTU/lb-°FGas
Thermal Conductivity 0.117 W/m-K
@Temperature 20.0 °C
0.812 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -40.0 °C-40.0 °F
Boiling Point 172.95 °C343.31 °F
Heat of Formation -184.5 kJ/mol-184.5 kJ/molLiquid
 -139.3 kJ/mol-139.3 kJ/molGas
 
Descriptive Properties
CAS registry number (CARN)7789-60-8
Chemical FormulaPBr3
SolubilityReacts with H2O and EtOH; Soluble in Acetone and CS2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphorus (V) Oxychloride, POCl3
Phosphorus (V) Oxybromide, POBr3
Phosphorus (III) Chloride, PCl3
Phosphorous (V) Chloride, PCl5
Phosphorous (V) Bromide, PBr5

EINOR2922 / 5029

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.