System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Rogers Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate
Categories:
Polymer
;
Thermoset
;
Silicone
;
Silicone Rubber
;
Silicone, Molded, Glass Fiber Filled
Material Notes:
Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE
Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.35
g/cc
1.35
g/cc
silicone property; Arlon SQA-TMS-024
Thickness
76.2
microns
3.00
mil
side 1 silicone; Arlon SQA-TMS-003
203
microns
8.00
mil
substrate; Arlon SQA-TMS-003
229
microns
9.00
mil
side 2 silicone; Arlon SQA-TMS-003
508
microns
20.0
mil
overall; Arlon SQA-TMS-003
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
60
60
silicone property; ASTM D2240
Tensile Strength, Ultimate
5.52
MPa
800
psi
silicone property; ASTM D412
Elongation at Break
225 %
225 %
silicone property; ASTM D412
Adhesive Bond Strength
0.0558
MPa
8.10
psi
Arlon SQA-TMS-011
Tear Strength
15.8
kN/m
90.0
pli
silicone property; ASTM D624
Electrical Properties
Metric
English
Comments
Dielectric Strength
23.6
kV/mm
600
kV/in
ASTM D149
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
232
°C
450
°F
Minimum Service Temperature, Air
-56.7
°C
-70.0
°F
Processing Properties
Metric
English
Comments
Cure Time
15.0
min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250
hour
@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life
6.00
Month
@Temperature 23.9 °C
6.00
Month
@Temperature 75.0 °F
Descriptive Properties
Color
Red
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Rogers Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 56976B026 Silicone Rubber/Fiberglass Laminate
Fiberglass Grade B
Rogers Arlon 51141R015 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51228R025 Silicone Rubber/Fiberglass Laminate
PARL016 / 79668
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.