MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 1501 Polyester, Briquette, Compression Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength values. UL recognized under component file E40654. 01501 is available in gray, blue, or tan color.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.680 g/cc0.0246 lb/in³ASTM D1895
Density 1.89 g/cc0.0683 lb/in³ASTM D792
Water Absorption 0.299 %0.299 %ASTM D570
Linear Mold Shrinkage 0.0031 cm/cm0.0031 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7070ASTM D785
Tensile Strength, Ultimate 43.0 MPa6240 psiASTM D638
Elongation at Break 0.57 %0.57 %ASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 91.0 MPa13200 psiASTM D790
Flexural Modulus 10.8 GPa1570 ksiASTM D790
Compressive Strength 153 MPa22200 psiASTM D695
Izod Impact, Notched 0.248 J/cm0.465 ft-lb/inASTM D256
Charpy Impact, Notched 0.265 J/cm²1.26 ft-lb/in²ASTM D256
Impact 137137J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+14 ohm-cm3.20e+14 ohm-cmASTM D247
Dielectric Constant 5.35.3ASTM D150
Dielectric Strength 10.3 kV/mm262 kV/inStep by Step; ASTM D149
 12.6 kV/mm320 kV/inShort Time; ASTM D149
Dielectric Breakdown 20200 V20200 V1hr 94C; ASTM D149
Dissipation Factor 0.02780.0278ASTM D150
Arc Resistance 190 sec190 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.700 W/m-K
@Temperature 100 °C
4.86 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 167 °C333 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 24 %24 %ASTM D2863
Shrinkage 0.043 %0.043 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1500 Polyester, Granular, Transfer Molded
Plenco 1500 Polyester, Granular, Compression Molded
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded

PLEL13 / 50581

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.