MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Diamonex DLC Diamond Like Carbon Coating
Categories: Carbon; Diamond

Material Notes: Superhard, conformal and low friction coating of amorphous carbon with diamond-like bonds.

Prime Features:

  • Wear/abrasion resistant
  • Low Friction
  • High surface hardness
  • Corrosion resistance
  • Conformal coatings
  • Biocompatible
Typical Markets:
  • Aerospace
  • Electronics
  • Industrial
  • Medical/Dental
  • Optics
  • Semiconductor
  • Transportation
Production Capabilities:
  • Coatings for metals, ceramics, plastics, glass
  • Flat and 3 dimensional part processing capability
  • RF and Ion Beam direct deposition(PECVD)
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 0.00500 - 30.0 microns0.000197 - 1.18 milcoating
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction <= 0.1<= 0.1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 - 1.00e+12 ohm-cm1.00e+6 - 1.00e+12 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 - 450 °C662 - 842 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 150 °C<= 302 °FDeposition Temperature
 
Descriptive Properties
Chemical Resistanceinert
Hardness8 to 25 GPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BACT DLC Diamond-Like Coating
Eifeler Coatings Technology SUCASLIDE® DLC coating
Diamond, Polycrystalline
Cast Stainless Steel 17- 4, UNS J92150 (Compostion Spec)
Diamond, Synthetic

CMORF5073 / 200311

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.