MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow XU 32046.31 Barrier Polymer
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Polyvinyl Dichloride (PVDC)

Material Notes: Excellent oxygen and water vapor barrier

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccDow Method
Bulk Density 0.801 g/cc0.0289 lb/in³Dow Method
Particle Size 280 µm280 µmDow Method
Moisture Vapor Transmission 0.0315 cc-mm/m²-24hr-atm0.0800 cc-mil/100 in²-24hr-atmblown film sample; ASTM F1249-90
Oxygen Transmission 0.0433 cc-mm/m²-24hr-atm0.110 cc-mil/100 in²-24hr-atmblown film sample; ASTM D3985-81
 
Thermal PropertiesMetricEnglishComments
Melting Point 158 °C316 °FDow Method (DSC)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow XU 32019.10 Barrier Polymer
SK Chemicals Saran® MA 119 PVDC
SK Chemicals Saran® 168
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
SK Chemicals Saran® 506 Polymer

PDOW1485 / 30703

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.