MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled

Material Notes: Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low warp and resistance to sink-mark formation. It maintains its inherent chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³dry; ISO 1183
Water Absorption 1.1 %1.1 %24 hour; ISO Test
 5.7 %5.7 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.6 %1.6 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi0.2 in/min; ASTM Test
 27.0 MPa
@Temperature 120 °C
3920 psi
@Temperature 248 °F
ISO Data
 27.0 MPa
@Temperature 120 °C
3920 psi
@Temperature 248 °F
ASTM Test
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ASTM Test
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ISO Data
 135 MPa
@Temperature -40.0 °C
19600 psi
@Temperature -40.0 °F
ASTM Test
 135 MPa
@Temperature -40.0 °C
19600 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Ultimate 60.0 MPa8700 psi5mm/min; ISO 527
Elongation at Break 30 %30 %5mm/min; ISO 527
 30 %30 %0.2 in/min; ASTM Test
 5.0 %
@Temperature -40.0 °C
5.0 %
@Temperature -40.0 °F
ASTM Test
 5.0 %
@Temperature -40.0 °C
5.0 %
@Temperature -40.0 °F
ISO Data
 30 %
@Temperature 80.0 °C
30 %
@Temperature 176 °F
ASTM Test
 30 %
@Temperature 80.0 °C
30 %
@Temperature 176 °F
ISO Data
 40 %
@Temperature 120 °C
40 %
@Temperature 248 °F
ASTM Test
 40 %
@Temperature 120 °C
40 %
@Temperature 248 °F
ISO Data
Tensile Modulus 3.80 GPa551 ksi1mm/min; ISO 527
 1.20 GPa
@Temperature 120 °C
174 ksi
@Temperature 248 °F
ISO Data
 1.40 GPa
@Temperature 80.0 °C
203 ksi
@Temperature 176 °F
ISO Data
 7.70 GPa
@Temperature -40.0 °C
1120 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 50.0 MPa7250 psiISO Data
Flexural Modulus 2.10 GPa305 ksiISO Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 95.0 °C203 °FInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
 X
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8260 HS PA6 (Conditioned)
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry)
BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned)
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® 8253 HS BK-102 PA6 (Dry)

PBASF9184 / 84948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.