MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Delcrome® 93 White Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; White Cast Iron

Material Notes: Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high hardness and wear resistance. Mo and Co content make heat resistance better than other irons.

Processing: Anneal: 6hours/790°C (1450°F), furnace cool; Harden: 2 hours/1065°C (1950°F), air cooled. Temper: 2 hours/190°C (375°F). As cast preferable, should be ground to size or E.D.M. Annealing for other machining operations is not reliable. Difficult to anneal and harden.

Corrosion Resistance: Generally superior to mild steel, but worse than 410 stainless steel. Significant corrosion in weak acids and will pit in the presence of chloride.

Applications: Abrasive metal-on-metal applications below 590°C (1100°F); agricultural implements, sealrings, brick making die parts, cement feed shoes, ice scraper blades, sand mixers, drill collars, and other low impact applications

Forms: Simple cast shapes, preferably chill cast, comparable hardfacing consumables.

Product of former Deloro Stellite Inc. Similar to Delfer B

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.77 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 650 - 807650 - 807
 113
@Temperature 900 °C
113
@Temperature 1650 °F
Hot Hardness
 476
@Temperature 600 °C
476
@Temperature 1110 °F
Hot Hardness
 612
@Temperature 400 °C
612
@Temperature 752 °F
Hot Hardness
Hardness, Knoop 729 - 906729 - 906Converted from Brinell hardness
Hardness, Rockwell C 58 - 6558 - 65
Hardness, Vickers 700 - 871700 - 871Converted from Brinell
Tensile Strength, Ultimate 414 MPa60000 psi
Elongation at Break <= 1.0 %<= 1.0 %much less than 1%
Modulus of Elasticity 240 GPa34800 ksi
Izod Impact <= 1.00 J<= 0.738 ft-lb
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.75 µm/m-°C
@Temperature 20.0 - 100 °C
4.31 µin/in-°F
@Temperature 68.0 - 212 °F
 10.0 µm/m-°C
@Temperature 20.0 - 900 °C
5.56 µin/in-°F
@Temperature 68.0 - 1650 °F
 10.2 µm/m-°C
@Temperature 20.0 - 300 °C
5.67 µin/in-°F
@Temperature 68.0 - 572 °F
 11.1 µm/m-°C
@Temperature 20.0 - 500 °C
6.17 µin/in-°F
@Temperature 68.0 - 932 °F
 11.5 µm/m-°C
@Temperature 20.0 - 700 °C
6.39 µin/in-°F
@Temperature 68.0 - 1290 °F
Thermal Conductivity 11.3 W/m-K78.4 BTU-in/hr-ft²-°F
Melting Point 1138 - 1220 °C2080 - 2220 °F
Solidus 1138 °C2080 °F
Liquidus 1215 °C2219 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.3 %3.3 %
Chromium, Cr 18 %18 %
Cobalt, Co 6.3 %6.3 %
Iron, Fe 53.5 %53.5 %
Molybdenum, Mo 16 %16 %
Silicon, Si 0.90 %0.90 %
Vanadium, V 2.0 %2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Delcrome® 90 White Cast Iron
Haynes Stellite Alloy No. 27 cast, (UNS R30027) Superalloy
Stellite Alloy No. 21 cast (UNS R30021) Superalloy
ASTM class 35 Standard gray iron test bars, as cast
ASTM class 40 Standard gray iron test bars, as cast

NSJNAC / 19193

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.