MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel Aquamet® 17 Martensitic Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Precipitation Hardening Stainless

Material Notes: AQUAMET 17 is a precipitation-hardening, martensitic stainless steel. Because it is hardened by a heat treatment, it provides high strength regardless of the diameter. It also offers good toughness and corrosion resistance. A popular choice, AQUAMET 17 is widely used in pleasure boats, ski boats, workboats, fishing trawlers, and crew boats, as well as pilot and patrol boats.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 931 MPa135000 psi
Tensile Strength, Yield 724 MPa
@Strain 0.2 %
105000 psi
@Strain 0.2 %
Tension
Elongation at Break 12 %12 %in 2"; 8" to 12"
 16 %
@Thickness <=203 mm
16 %
@Thickness <=8.00 in
in 2"
Reduction of Area  35 %
@Thickness 203 - 305 mm
35 %
@Thickness 8.00 - 12.0 in
 50 %
@Thickness <=203 mm
50 %
@Thickness <=8.00 in
Shear Strength 483 MPa
@Strain 0.2 %
70000 psi
@Strain 0.2 %
Torsion
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.070 %<= 0.070 %
Chromium, Cr 14.5 - 16.5 %14.5 - 16.5 %
Copper, Cu 3.0 - 5.0 %3.0 - 5.0 %
Iron, Fe >= 70.903 %>= 70.903 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Nb + Ta 0.15 - 0.45 %0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %3.0 - 5.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel Aquamet® 22 Stainless Steel
Crucible Steel Aquamet® 19 Stainless Steel
Type 431 Martensitic Stainless Steel, Intermediate Temper Forgings, UNS S43100
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536
Special Metals INCONEL® HX Nickel Superalloy (UNS N06002)

NCRUC028 / 16021

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.