MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aclo Accutech Polypropylene Homopolymer HP0339T20L Talc Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inMD; ASTM D955
Melt Flow 21 g/10 min21 g/10 minASTM D1238
Ash 20 %20 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
Elongation at Break 18 %18 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 2.099 GPa304.5 ksiASTM D638
Flexural Strength 45.0 MPa6530 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 0.251 J/cm0.470 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C144 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Total PPR 7425 Polypropylene, Injection Molding Grade
Aclo Accutech Polypropylene Copolymer CP0436T20L Talc Reinforced
A. Schulman ComAlloy Hiloy® 125 Polypropylene, Glass Reinforced, Chemically Coupled
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced

PACLO256 / 22511

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.