MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no particle breakdown during thermal cycling and provide dust-free performance. Type ZOG is useful at temperatures up to 2400°C under oxidizing conditions with no sintering or particle breakdown and minimal sticking.

Zircar Zirconia Single Crystal Grog Type ZOG was developed for RF (Radio Frequency) induction furnaces operating above 2000°C. These furnaces are typically used in fiber optic draw towers and crystal growing applications where high purity, low electrical conductivity and dust-free performance at extreme temperatures are essential. Zirconia Single Crystal Grog Type ZOG is free flowing, therefore conforming to irregular configurations to fill small and intricate areas.

Type ZOG contains no organic binders and will produce no smoke or odor when heated and is available in two particle size ranges.

  • Type ZOG-1 has a Tyler mesh size of -8 to +14 (2.4mm to 1.2mm)
  • Type ZOG-2 has a Tyler mesh size of -10 to +28 (1.7mm to 0.6mm).

Features:

  • High Purity ZrO2 Single Crystal (99%+)
  • High Temperature Stability to 2400°C
  • Low Thermal Conductivity
  • Two Particle Size Ranges are Offered
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Virtually Dust Free Performance
  • Available ‘Off the Shelf’

Application Information:

  • ZOG Grog is used as insulation and crucible support in crystal growing furnaces.
  • ZOG Grog is used as insulation for glass melting and fiber optic draw furnaces.
  • ZOG Grog is used as bulk fill insulation.
  • ZOG Grog is used as ultra high temperature insulation for advanced energy systems.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.75 g/cc0.0994 lb/in³
Outgassing - Total Mass Loss 0.00 %0.00 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 2715 °C4919 °F
Maximum Service Temperature, Air 2400 °C4350 °F
Shrinkage 0.00 %
@Temperature 2400 °C,
Time 1800 sec
0.00 %
@Temperature 4350 °F,
Time 0.500 hour
 
Component Elements PropertiesMetricEnglishComments
HfO2 1.0 - 2.0 %1.0 - 2.0 %
SiO2 0.15 %0.15 %
TiO2 0.15 %0.15 %
ZrO2 97 - 98 %97 - 98 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating

C6ZIR010 / 2766

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.