MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC LUMIFLON® FE-4400 for Coil Coating Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON fluoropolymer resins were developed in 1982 as the first solvent-soluble fluoropolymers in the world. LUMIFLON polymers consist of alternating fluoroethylene and alkyl vinyl ether segments (FEVE). The fluorinated segments provide outstanding UV stability, weather resistance, and chemical resistance, while the vinyl ether segments provide solvent compatibility and cross-linking sites. LUMIFLON resins are used to make ultra-weatherable coatings for architectural, aerospace, automotive, and industrial maintenance markets. LUMIFLON FE-4400 is a water emulsion product that was developed to meet VOC and HAPS regulations on many solvents in the U. S. FE-4400 is hydroxyl functional, and can be crosslinked with water-dispersible polyisocyanates. Like other LUMIFLON resins, FE-4400 is used to produce coatings with high gloss and excellent weatherability. This bulletin describes the use of FE-4400 to produce single component elevated cure coatings. These coatings are primarily coil coatings for architectural applications.

Product Characteristics:

  • Moderate OH functionality
  • Excellent weathering and chemical resistance
  • Suitable for ambient cure and bake coatings
  • Used in architectural ambient cure and coil coatings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Solids Content 50 %50 %
Particle Size 0.10 - 0.20 µm0.10 - 0.20 µm
pH 7.0 - 9.07.0 - 9.0
 
Mechanical PropertiesMetricEnglishComments
Impact  >= 0.50
@Diameter 12.7 mm
>= 0.50
@Diameter 0.500 in
[m], Intrusion 0.5 kg; ISO 6272
 >= 0.50
@Diameter 12.7 mm
>= 0.50
@Diameter 0.500 in
[m], Extrusion 0.5 kg; ISO 6272
 
Optical PropertiesMetricEnglishComments
Gloss 65 %65 %20°; ISO 2813
 82 %82 %60°; ISO 2813
 
Processing PropertiesMetricEnglishComments
Cure Time  600 min
@Temperature 40.0 °C
10.0 hour
@Temperature 104 °F
Flashing
 1800 min
@Temperature 150 °C
30.0 hour
@Temperature 302 °F
Baking
 
Descriptive Properties
AppearanceMilky White Liquid
Hardness4HPencil, ASTM D3363
Ionic CharacterAnionic
Minimum Film Forming Temperature55°C
OH Number49[mg KOH/g]-polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy
Dymax EMAX 10006 Voil Coil Assembly Disk Drive Adhesive
Dymax EMAX 10002 Voil Coil Assembly Disk Drive Adhesive
Dymax 930 Coil Terminating, Tamper proofing and Structural Electronic Bonder
Dymax 928 Coil Terminating, Tamper proofing and Structural Electronic Bonder

PAGCX115 / 191224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.