Teflon™ PFA C-980 (perfluoroalkoxy) fluoropolymer resins combine the chemical and high temperature resistance of Teflon™ PFA with anti-static levels of electrical conductivity. Anti-static linings of components used in the chemical processing industries; industrial film; articles requiring superior electrical, chemical, and thermal properties.Information provided by Chemours. |