MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Armstrong A-2/W Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Activators W or H-20 has a very low thermal expansion coefficient, especially important for bonding ceramics, porcelain, etc. A-2 with Activator A is qualified under Mil. Spec. MIL-A-47284 (MI).

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 130000 cP130000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Ultimate 42.7 MPa6200 psiafter optimum cure
Elongation at Break 3.1 %3.1 %
Adhesive Bond Strength 39.0 MPa5650 psiSteel-Steel; after optimum cure
 8.27 MPa
@Temperature 82.2 °C
1200 psi
@Temperature 180 °F
Aluminum-Aluminum tensile shear
 20.0 MPa
@Temperature -54.4 °C
2900 psi
@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
 37.6 MPa
@Temperature 25.0 °C
5450 psi
@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
 
Thermal PropertiesMetricEnglishComments
CTE, linear 86.0 µm/m-°C
@Temperature 20.0 °C
47.8 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 22.2 °C72.0 °F
 93.3 °C200 °FOptimum cure is 30 min. @ 200°F
 149 °C300 °FFast cure is 5 min. @ 300°F
Pot Life <= 60.0 min
@Temperature 25.0 °C
<= 60.0 min
@Temperature 77.0 °F
100 g
 
Descriptive Properties
ColorWhite
Mix Ratio3/1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armstrong A-2/A Epoxy Adhesive
Armstrong A-2/E Epoxy Adhesive
H.C. Starck Amperit® 515.1 Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12
H.C. Starck Amperit® 518.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)

PARM06 / 24538

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.