MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AISI 1080 Steel, normalized at 900°C (1650°F), air cooled, 100 mm (4 in.) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; High Carbon Steel

Key Words: UNS G10800, AMS 5110, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1080), MIL SPEC MIL-S-16974, SAE J403, SAE J412, SAE J414
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 269269
Hardness, Knoop 294294Converted from Brinell
Hardness, Rockwell B 9999Converted from Brinell
Hardness, Rockwell C 2727Converted from Brinell
Hardness, Vickers 284284Converted from Brinell
Tensile Strength, Ultimate 931 MPa135000 psi
Tensile Strength, Yield 440 MPa63800 psi
Elongation at Break 10.7 %10.7 %in 50 mm
Reduction of Area 15.5 %15.5 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
Izod Impact 7.00 J5.16 ft-lbannealed at 790°C (1450°F)
 7.00 J5.16 ft-lbas rolled
 7.00 J5.16 ft-lbnormalized at 900°C (1650°F)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000180 ohm-cm
@Temperature 20.0 °C
0.0000180 ohm-cm
@Temperature 68.0 °F
 0.0000232 ohm-cm
@Temperature 100 °C
0.0000232 ohm-cm
@Temperature 212 °F
 0.0000308 ohm-cm
@Temperature 200 °C
0.0000308 ohm-cm
@Temperature 392 °F
 0.0000505 ohm-cm
@Temperature 400 °C
0.0000505 ohm-cm
@Temperature 752 °F
 0.0000772 ohm-cm
@Temperature 600 °C
0.0000772 ohm-cm
@Temperature 1110 °F
 0.0000935 ohm-cm
@Temperature 700 °C
0.0000935 ohm-cm
@Temperature 1290 °F
 0.0001129 ohm-cm
@Temperature 800 °C
0.0001129 ohm-cm
@Temperature 1470 °F
 0.0001164 ohm-cm
@Temperature 900 °C
0.0001164 ohm-cm
@Temperature 1650 °F
 0.0001246 ohm-cm
@Temperature 1250 °C
0.0001246 ohm-cm
@Temperature 2280 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 0.000 - 100 °C
6.11 µin/in-°F
@Temperature 32.0 - 212 °F
 11.5 µm/m-°C
@Temperature 0.000 - 200 °C
6.39 µin/in-°F
@Temperature 32.0 - 392 °F
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
 13.1 µm/m-°C
@Temperature 0.000 - 400 °C
7.28 µin/in-°F
@Temperature 32.0 - 752 °F
 13.7 µm/m-°C
@Temperature 0.000 - 500 °C
7.61 µin/in-°F
@Temperature 32.0 - 932 °F
 14.0 µm/m-°C
@Temperature 0.000 - 600 °C
7.78 µin/in-°F
@Temperature 32.0 - 1110 °F
 14.6 µm/m-°C
@Temperature 0.000 - 700 °C
8.11 µin/in-°F
@Temperature 32.0 - 1290 °F
Specific Heat Capacity  0.490 J/g-°C
@Temperature >=100 °C
0.117 BTU/lb-°F
@Temperature >=212 °F
 0.531 J/g-°C
@Temperature 150 - 200 °C
0.127 BTU/lb-°F
@Temperature 302 - 392 °F
 0.548 J/g-°C
@Temperature 200 - 250 °C
0.131 BTU/lb-°F
@Temperature 392 - 482 °F
 0.565 J/g-°C
@Temperature 250 - 300 °C
0.135 BTU/lb-°F
@Temperature 482 - 572 °F
 0.586 J/g-°C
@Temperature 300 - 350 °C
0.140 BTU/lb-°F
@Temperature 572 - 662 °F
 0.607 J/g-°C
@Temperature 350 - 400 °C
0.145 BTU/lb-°F
@Temperature 662 - 752 °F
 0.615 J/g-°C
@Temperature 750 - 800 °C
0.147 BTU/lb-°F
@Temperature 1380 - 1470 °F
 0.670 J/g-°C
@Temperature 450 - 500 °C
0.160 BTU/lb-°F
@Temperature 842 - 932 °F
 0.712 J/g-°C
@Temperature 550 - 600 °C
0.170 BTU/lb-°F
@Temperature 1020 - 1110 °F
 0.770 J/g-°C
@Temperature 650 - 700 °C
0.184 BTU/lb-°F
@Temperature 1200 - 1290 °F
 2.08 J/g-°C
@Temperature 700 - 750 °C
0.497 BTU/lb-°F
@Temperature 1290 - 1380 °F
Thermal Conductivity  24.4 W/m-K
@Temperature 800 °C
169 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 26.8 W/m-K
@Temperature 1000 °C
186 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 30.1 W/m-K
@Temperature 700 °C
209 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 30.1 W/m-K
@Temperature 1200 °C
209 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 32.7 W/m-K
@Temperature 600 °C
227 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 35.1 W/m-K
@Temperature 500 °C
244 BTU-in/hr-ft²-°F
@Temperature 932 °F
 38.1 W/m-K
@Temperature 400 °C
264 BTU-in/hr-ft²-°F
@Temperature 752 °F
 41.3 W/m-K
@Temperature 300 °C
287 BTU-in/hr-ft²-°F
@Temperature 572 °F
 45.2 W/m-K
@Temperature 200 °C
314 BTU-in/hr-ft²-°F
@Temperature 392 °F
 47.7 W/m-K
@Temperature 0.000 °C
331 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 48.1 W/m-K
@Temperature 100 °C
334 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.75 - 0.88 %0.75 - 0.88 %
Iron, Fe 98.13 - 98.65 %98.13 - 98.65 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel
AISI 8620 Steel, mock carburized, reheated and oil quenched, 230°C (450°F) temper, 100 mm (4 in.) round
AISI 1080 Steel, as rolled
AISI 1080 Steel, annealed at 790°C (1450°F)
AISI 8620 Steel, normalized, 100 mm (4 in.) round

M1080L / 7088

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.