Features and Typical Applications Provide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conductivity. Typical applications include a wide range of electrical components such as capacitors and transformers.
Emerson & Cuming 2057FR/11 Stycast® Two-Component Epoxy Flame Retardant Encapsulant
- Low Viscosity
- Good Chemical Resistance
- Filled
- High Temperature
- Mix Ratio by Weight = 100:8
Cure Type: Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |