MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cosmic Plastics K66/6230F Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled

Material Notes: Description: Cosmic K66 / 6230F is a long glass fiber filled, flame retardant, general purpose diallyl iso-phthalate molding compound which is supplied in a flake form. It can be preformed and molds easily in standard compression or transfer equipment. It has passed NASA outgassing tests.

Features: It has excellent mechanical and electrical properties with a high dielectric strength and low dielectric constant. It has superior heat resistance and excellent machining qualities.

Applications: The high strength of this material makes it ideal for switches, terminals, housings, structural parts and insulators.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/cc
Bulk Factor 6.06.0
Water Absorption 0.25 %
@Temperature 50.0 °C,
Time 173000 sec
0.25 %
@Temperature 122 °F,
Time 48.0 hour
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.4 - 68.9 MPa6000 - 10000 psi
Flexural Strength 89.6 - 117 MPa13000 - 17000 psi
Compressive Strength 165 - 207 MPa24000 - 30000 psi
Izod Impact, Notched 1.60 - 3.20 J/cm3.00 - 6.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm
 3.00e+10 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
3.00e+10 ohm-cm
@Temperature 158 °F,
Time 720 hour
100% RH
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohm
 5.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
5.00e+10 ohm
@Temperature 158 °F,
Time 720 hour
100% RH
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dry
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Wet
 4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
Wet
 40
@Frequency 1000 Hz
40
@Frequency 1000 Hz
Dry
Dielectric Strength 15.7 kV/mm400 kV/inWet, step by step
 18.7 kV/mm475 kV/inDry, step by step
Dielectric Breakdown 60 V60 VWet, step by step
 64 V64 VDry, step by step
Dissipation Factor  0.0080
@Frequency 1000 Hz
0.0080
@Frequency 1000 Hz
Dry
 0.0090
@Frequency 1000 Hz
0.0090
@Frequency 1000 Hz
Wet
 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
Dry
 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
Wet
Arc Resistance 180 sec180 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 24.0 µm/m-°C
@Temperature -40.0 - 100 °C
13.3 µin/in-°F
@Temperature -40.0 - 212 °F
Heat Distortion Temperature 260 °C500 °F
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 135 - 170 °C275 - 338 °F
 
Descriptive Properties
Dimensional Stability<0.01%
MIL-M-14GII-30FASTM D5948-96
Molding Pressure500-8000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy
Raschig Group 6552 DAIP
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
Cosmic Plastics K77/6220F Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound

PCOSM014 / 190796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.