Physical Properties | Metric | English | Comments |
---|
Density | 1.23 - 1.73 g/cc | 0.0444 - 0.0625 lb/in³ |
| 1.20 - 1.30 g/cc @Temperature 245 - 295 °C | 0.0434 - 0.0470 lb/in³ @Temperature 473 - 563 °F |
Filler Content | 10.0 - 45.0 % | 10.0 - 45.0 % |
Water Absorption | 0.350 - 6.00 % | 0.350 - 6.00 % |
Moisture Absorption at Equilibrium | 0.700 - 2.00 % | 0.700 - 2.00 % |
Viscosity | 30.0 - 120 cP @Temperature 280 - 300 °C | 30.0 - 120 cP @Temperature 536 - 572 °F |
| 30.0 - 120 cP @Shear Rate 100 - 1000 1/s | 30.0 - 120 cP @Shear Rate 100 - 1000 1/s |
Maximum Moisture Content | 0.0200 - 0.200 | 0.0200 - 0.200 |
Linear Mold Shrinkage | 0.000500 - 0.0500 cm/cm | 0.000500 - 0.0500 in/in |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in |
Melt Flow | 2.00 - 44.4 g/10 min | 2.00 - 44.4 g/10 min |
Ash | 20.0 - 48.0 % | 20.0 - 48.0 % |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell M | 74.0 - 99.0 | 74.0 - 99.0 |
Hardness, Rockwell R | 112 - 122 | 112 - 122 |
Tensile Strength, Ultimate | 50.0 - 195 MPa | 7250 - 28300 psi |
| 25.0 - 70.0 MPa @Temperature 60.0 - 150 °C | 3630 - 10200 psi @Temperature 140 - 302 °F |
Tensile Strength, Yield | 71.7 - 175 MPa | 10400 - 25400 psi |
Elongation at Break | 1.00 - 160 % | 1.00 - 160 % |
| 2.70 - 20.0 % @Temperature 60.0 - 150 °C | 2.70 - 20.0 % @Temperature 140 - 302 °F |
Elongation at Yield | 2.00 - 6.00 % | 2.00 - 6.00 % |
| 5.00 - 10.0 % @Temperature 90.0 - 150 °C | 5.00 - 10.0 % @Temperature 194 - 302 °F |
Modulus of Elasticity | 3.30 - 15.5 GPa | 479 - 2250 ksi |
| 2.60 - 8.00 GPa @Temperature 60.0 - 150 °C | 377 - 1160 ksi @Temperature 140 - 302 °F |
Flexural Yield Strength | 90.0 - 285 MPa | 13100 - 41300 psi |
Flexural Modulus | 2.90 - 12.5 GPa | 421 - 1810 ksi |
Compressive Yield Strength | 138 - 255 MPa | 20000 - 37000 psi |
Poissons Ratio | 0.340 - 0.400 | 0.340 - 0.400 |
Izod Impact, Notched | 0.300 - 1.33 J/cm | 0.562 - 2.50 ft-lb/in |
| 0.420 - 0.420 J/cm @Temperature -40.0 - -40.0 °C | 0.787 - 0.787 ft-lb/in @Temperature -40.0 - -40.0 °F |
Izod Impact, Unnotched | 0.427 - 9.08 J/cm | 0.800 - 17.0 ft-lb/in |
| 5.50 - 5.50 J/cm @Temperature -40.0 - -40.0 °C | 10.3 - 10.3 ft-lb/in @Temperature -40.0 - -40.0 °F |
Izod Impact, Notched (ISO) | 2.60 - 42.0 kJ/m² | 1.24 - 20.0 ft-lb/in² |
| 3.00 - 10.0 kJ/m² @Temperature -40.0 - -30.0 °C | 1.43 - 4.76 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Izod Impact, Unnotched (ISO) | 4.00 - 55.0 kJ/m² | 1.90 - 26.2 ft-lb/in² |
| 3.40 - 50.0 kJ/m² @Temperature -40.0 - -30.0 °C | 1.62 - 23.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Charpy Impact Unnotched | 2.00 - 9.00 J/cm² | 9.52 - 42.8 ft-lb/in² |
| 2.00 - 6.00 J/cm² @Temperature -40.0 - -20.0 °C | 9.52 - 28.6 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Charpy Impact, Notched | 0.200 - 1.60 J/cm² | 0.952 - 7.61 ft-lb/in² |
| 0.200 - 1.00 J/cm² @Temperature -40.0 - -20.0 °C | 0.952 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Tensile Creep Modulus, 1 hour | 2300 - 7000 MPa | 334000 - 1.02e+6 psi |
Tensile Creep Modulus, 1000 hours | 1500 - 6000 MPa | 218000 - 870000 psi |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm | 1.00e+9 - 1.00e+17 ohm-cm |
Surface Resistance | 1.00e+10 - 5.00e+14 ohm | 1.00e+10 - 5.00e+14 ohm |
Dielectric Constant | 3.00 - 13.9 | 3.00 - 13.9 |
Dielectric Strength | 15.7 - 41.0 kV/mm | 400 - 1040 kV/in |
Dissipation Factor | 0.0100 - 0.540 | 0.0100 - 0.540 |
Dielectric Loss Index | 0.0150 - 0.150 | 0.0150 - 0.150 |
Arc Resistance | 125 - 140 sec | 125 - 140 sec |
Comparative Tracking Index | 375 - 600 V | 375 - 600 V |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 10.0 - 55.8 µm/m-°C | 5.56 - 31.0 µin/in-°F |
| 31.0 - 31.0 µm/m-°C @Temperature 55.0 - 160 °C | 17.2 - 17.2 µin/in-°F @Temperature 131 - 320 °F |
| 18.5 - 24.0 µm/m-°C @Temperature 35.0 - 55.0 °C | 10.3 - 13.3 µin/in-°F @Temperature 95.0 - 131 °F |
| 18.5 - 24.0 µm/m-°C @Thickness 2.00 - 2.00 mm | 10.3 - 13.3 µin/in-°F @Thickness 0.0787 - 0.0787 in |
CTE, linear, Transverse to Flow | 46.0 - 100 µm/m-°C | 25.6 - 55.6 µin/in-°F |
| 127 - 127 µm/m-°C @Temperature 55.0 - 160 °C | 70.6 - 70.6 µin/in-°F @Temperature 131 - 320 °F |
Specific Heat Capacity | 1.90 - 2.29 J/g-°C @Temperature 245 - 295 °C | 0.454 - 0.547 BTU/lb-°F @Temperature 473 - 563 °F |
Thermal Conductivity | 0.350 - 0.504 W/m-K | 2.43 - 3.50 BTU-in/hr-ft²-°F |
| 0.210 - 0.270 W/m-K @Temperature 245 - 295 °C | 1.46 - 1.87 BTU-in/hr-ft²-°F @Temperature 473 - 563 °F |
Melting Point | 220 - 275 °C | 428 - 527 °F |
Maximum Service Temperature, Air | 115 - 254 °C | 239 - 489 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 203 - 260 °C | 397 - 500 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 - 257 °C | 158 - 495 °F |
Vicat Softening Point | 200 - 255 °C | 392 - 491 °F |
Glass Transition Temp, Tg | 70.0 - 90.0 °C | 158 - 194 °F |
Flammability, UL94 | HB - V-0 | HB - V-0 |
Flame Spread | 0.000 - 80.0 mm/min | 0.000 - 3.15 in/min |
Oxygen Index | 24.0 - 36.0 % | 24.0 - 36.0 % |
Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 260 - 300 °C | 500 - 572 °F |
Nozzle Temperature | 254 - 310 °C | 489 - 590 °F |
Melt Temperature | 220 - 310 °C | 428 - 590 °F |
Mold Temperature | 26.7 - 121 °C | 80.0 - 250 °F |
Drying Temperature | 60.0 - 130 °C | 140 - 266 °F |
Moisture Content | 0.0300 - 0.200 % | 0.0300 - 0.200 % |
Injection Pressure | 3.50 - 138 MPa | 508 - 20000 psi |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.