MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems Accura® PEAK™
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Stiff plastic material for heat-resistant components

Features:

  • High heat resistance
  • Very high rigidity and stiffness
  • Excellent humidity/moisture resistance

Information provided by 3D Systems

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Leaders in providing fast Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA printing technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density  1.32 g/cc
@Temperature 25.0 °C
0.0477 lb/in³
@Temperature 77.0 °F
Liquid
 1.36 g/cc
@Temperature 25.0 °C
0.0491 lb/in³
@Temperature 77.0 °F
Solid
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Strength 57.0 - 78.0 MPa8270 - 11300 psiASTM D638
Elongation at Break 1.3 - 2.5 %1.3 - 2.5 %ASTM D638
Tensile Modulus 4.22 - 4.79 GPa612 - 695 ksiASTM D638
Flexural Strength 77.0 - 126 MPa11200 - 18300 psiASTM D790
Flexural Modulus 4.18 - 4.79 GPa606 - 695 ksiASTM D790
Izod Impact, Notched 0.213 - 0.273 J/cm0.399 - 0.511 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear  48.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
26.7 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-93
 92.0 µm/m-°C
@Temperature 50.0 - 120 °C
51.1 µin/in-°F
@Temperature 122 - 248 °F
ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °FUV Postcure Only; ASTM D648
 153 °C307 °F120 °C thermal postcure; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C138 °FUV Postcure Only; ASTM D648
 124 °C255 °F120 °C thermal postcure; ASTM D648
Glass Transition Temp, Tg 80.0 °C176 °FUV Postcure Only
 90.0 - 95.0 °C194 - 203 °F120 °C thermal postcure
 
Descriptive Properties
ColorTranslucent Amber
Critical Exposure11.5 mJ/cm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Bayblend® FR3040 PC/ABS Blend
VICTREX™ PEEK 450G™ General Purpose
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled

PAPPR201 / 206147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.