MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem HC7260LS-L HDPE Injection Molding Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its applications include: industrial containers, safety helmets, toilet seats, housewares, toys, lids, pallets, and boxes for beverage bottles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³ASTM-D792
ESCR 100% Igepal® <= 4.0 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
<= 4.0 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 7.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM-D2240
Tensile Strength, Yield 30.0 MPa4350 psiASTM-D638
Elongation at Yield 7.5 %7.5 %ASTM-D638
Flexural Modulus, 1% Secant 1350 MPa196000 psiASTM-D790
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °FASTM-D648
Vicat Softening Point 126 °C
@Load 1.02 kg
259 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HA7260 HDPE Injection Molding Polyethylene
Braskem H 306 Injection Molding Polypropylene
Braskem HD7255LS-L HDPE Injection Molding Polyethylene
Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer

PBRAS896 / 106742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.