MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.51 g/cc0.0361 - 0.0546 lb/in³Average value: 1.21 g/cc Grade Count:39
Filler Content 5.00 - 15.0 %5.00 - 15.0 %Average value: 8.64 % Grade Count:7
Water Absorption 0.0100 - 0.300 %0.0100 - 0.300 %Average value: 0.268 % Grade Count:18
Additive Loading 5.00 - 20.0 %5.00 - 20.0 %Average value: 12.5 % Grade Count:6
Linear Mold Shrinkage 0.00300 - 0.0170 cm/cm0.00300 - 0.0170 in/inAverage value: 0.00579 cm/cm Grade Count:35
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80.0 - 11280.0 - 112Average value: 100 Grade Count:3
Tensile Strength, Ultimate 27.6 - 45.0 MPa4000 - 6530 psiAverage value: 36.2 MPa Grade Count:24
Tensile Strength, Yield 32.4 - 50.3 MPa4700 - 7300 psiAverage value: 46.3 MPa Grade Count:17
Elongation at Break 1.00 - 10.0 %1.00 - 10.0 %Average value: 4.06 % Grade Count:37
Elongation at Yield 2.00 - 4.00 %2.00 - 4.00 %Average value: 2.60 % Grade Count:4
Modulus of Elasticity 2.28 - 3.10 GPa330 - 450 ksiAverage value: 2.56 GPa Grade Count:20
Flexural Yield Strength 8.96 - 89.6 MPa1300 - 13000 psiAverage value: 69.5 MPa Grade Count:36
Flexural Modulus 1.14 - 6.21 GPa165 - 900 ksiAverage value: 3.23 GPa Grade Count:37
Izod Impact, Notched 0.267 - 1.60 J/cm0.500 - 3.00 ft-lb/inAverage value: 0.540 J/cm Grade Count:34
Izod Impact, Unnotched 1.07 - 4.30 J/cm2.00 - 8.06 ft-lb/inAverage value: 2.20 J/cm Grade Count:29
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.100 - 1.00e+10 ohm-cm0.100 - 1.00e+10 ohm-cmAverage value: 3.03e+8 ohm-cm Grade Count:34
Surface Resistance 1.00 - 1.00e+6 ohm1.00 - 1.00e+6 ohmAverage value: 114000 ohm Grade Count:38
Static Decay 0.100 - 2.00 sec0.100 - 2.00 secAverage value: 1.18 sec Grade Count:19
Shielding Effectiveness 20.0 - 108 dB20.0 - 108 dBAverage value: 67.3 dB Grade Count:18
 
Thermal PropertiesMetricEnglishComments
CTE, linear 61.2 - 84.6 µm/m-°C34.0 - 47.0 µin/in-°FAverage value: 81.0 µm/m-°C Grade Count:13
CTE, linear, Transverse to Flow 93.0 - 113 µm/m-°C51.7 - 63.0 µin/in-°FAverage value: 101 µm/m-°C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 107 °C185 - 225 °FAverage value: 98.0 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 141 °C130 - 285 °FAverage value: 98.8 °C Grade Count:26
Flammability, UL94 HB - V-0HB - V-0Grade Count:26
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 254 °C356 - 489 °FAverage value: 225 °C Grade Count:17
Mold Temperature 38.0 - 93.3 °C100 - 200 °FAverage value: 70.7 °C Grade Count:19
Drying Temperature 37.8 - 82.2 °C100 - 180 °FAverage value: 79.0 °C Grade Count:18
Moisture Content 0.0200 - 0.100 %0.0200 - 0.100 %Average value: 0.0893 % Grade Count:15
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:13
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled

O1129 / 77811

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.