MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.78 g/cc0.0524 - 0.0643 lb/in³Average value: 1.57 g/cc Grade Count:306
 1.40 - 1.40 g/cc
@Temperature 262 - 295 °C
0.0506 - 0.0506 lb/in³
@Temperature 504 - 563 °F
Average value: 1.40 g/cc Grade Count:2
Filler Content 45.0 - 50.0 %45.0 - 50.0 %Average value: 49.6 % Grade Count:45
Water Absorption 0.300 - 4.80 %0.300 - 4.80 %Average value: 1.66 % Grade Count:132
Moisture Absorption at Equilibrium 0.170 - 2.00 %0.170 - 2.00 %Average value: 1.19 % Grade Count:89
 1.05 - 1.50 %
@Temperature 70.0 - 70.0 °C
1.05 - 1.50 %
@Temperature 158 - 158 °F
Average value: 1.29 % Grade Count:12
Water Absorption at Saturation 0.200 - 7.00 %0.200 - 7.00 %Average value: 3.89 % Grade Count:82
Viscosity  8000 - 160000 cP
@Temperature 277 - 322 °C
8000 - 160000 cP
@Temperature 531 - 612 °F
Average value: 38100 cP Grade Count:1
 8000 - 160000 cP
@Frequency 10.0 - 10000 Hz
8000 - 160000 cP
@Frequency 10.0 - 10000 Hz
Average value: 38100 cP Grade Count:1
 20.0 - 450 cP
@Temperature 280 - 300 °C
20.0 - 450 cP
@Temperature 536 - 572 °F
Average value: 38100 cP Grade Count:2
 20.0 - 450 cP
@Shear Rate 10.0 - 10000 1/s
20.0 - 450 cP
@Shear Rate 10.0 - 10000 1/s
Average value: 38100 cP Grade Count:2
Viscosity Test 131 - 152 cm³/g1.31 - 1.52 dl/gAverage value: 139 cm³/g Grade Count:7
Viscosity Number 105 - 150 cm³/g1.05 - 1.50 dl/gAverage value: 136 cm³/g Grade Count:4
Maximum Moisture Content 0.0200 - 0.9000.0200 - 0.900Average value: 0.166 Grade Count:16
Linear Mold Shrinkage 0.000100 - 0.0200 cm/cm0.000100 - 0.0200 in/inAverage value: 0.00318 cm/cm Grade Count:215
 0.00100 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00100 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00200 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.00100 - 0.0125 cm/cm0.00100 - 0.0125 in/inAverage value: 0.00673 cm/cm Grade Count:133
 0.00400 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00500 in/in
@Temperature 176 - 176 °F
Average value: 0.00467 cm/cm Grade Count:6
Melt Flow 1.00 - 40.0 g/10 min1.00 - 40.0 g/10 minAverage value: 16.0 g/10 min Grade Count:24
Spiral Flow 54.0 - 536 cm21.3 - 211 inAverage value: 138 cm Grade Count:6
Ash 48.0 - 58.0 %48.0 - 58.0 %Average value: 51.6 % Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 97.0 - 12097.0 - 120Average value: 109 Grade Count:7
Hardness, Rockwell R 98.0 - 12598.0 - 125Average value: 120 Grade Count:37
Ball Indentation Hardness 131 - 340 MPa19000 - 49300 psiAverage value: 276 MPa Grade Count:55
Tensile Strength, Ultimate 50.0 - 392 MPa7250 - 56900 psiAverage value: 212 MPa Grade Count:243
 65.0 - 342.669 MPa
@Temperature -40.0 - 150 °C
9430 - 49700.1 psi
@Temperature -40.0 - 302 °F
Average value: 124 MPa Grade Count:12
 47.0 - 175 MPa
@Temperature 60.0 - 180 °C
6820 - 25400 psi
@Temperature 140 - 356 °F
Average value: 124 MPa Grade Count:3
 47.0 - 175 MPa
@Strain 0.750 - 15.0 %
6820 - 25400 psi
@Strain 0.750 - 15.0 %
Average value: 124 MPa Grade Count:3
Tensile Strength, Yield 23.5 - 265 MPa3410 - 38400 psiAverage value: 208 MPa Grade Count:64
 131 - 265 MPa
@Temperature -20.0 - 93.3 °C
19000 - 38400 psi
@Temperature -4.00 - 200 °F
Average value: 179 MPa Grade Count:2
Elongation at Break 1.00 - 8.00 %1.00 - 8.00 %Average value: 2.62 % Grade Count:277
 1.80 - 8.00 %
@Temperature -40.0 - 150 °C
1.80 - 8.00 %
@Temperature -40.0 - 302 °F
Average value: 4.15 % Grade Count:10
Elongation at Yield 1.00 - 6.00 %1.00 - 6.00 %Average value: 2.81 % Grade Count:17
Modulus of Elasticity 10.2 - 22.2 GPa1480 - 3210 ksiAverage value: 15.7 GPa Grade Count:222
 4.00 - 19.788 GPa
@Temperature -40.0 - 150 °C
580 - 2870.0 ksi
@Temperature -40.0 - 302 °F
Average value: 8.37 GPa Grade Count:9
Flexural Yield Strength 185 - 425 MPa26800 - 61600 psiAverage value: 319 MPa Grade Count:201
 175 - 455.054 MPa
@Temperature -40.0 - 149 °C
25400 - 66000.1 psi
@Temperature -40.0 - 300 °F
Average value: 270 MPa Grade Count:8
Flexural Modulus 7.90 - 17.5 GPa1150 - 2540 ksiAverage value: 13.9 GPa Grade Count:216
 6.60 - 19.0985 GPa
@Temperature -40.0 - 149 °C
957 - 2770.04 ksi
@Temperature -40.0 - 300 °F
Average value: 10.8 GPa Grade Count:9
Flexural Strain at Break 3.00 - 5.00 %3.00 - 5.00 %Average value: 3.79 % Grade Count:7
Compressive Yield Strength 186 - 215 MPa27000 - 31200 psiAverage value: 198 MPa Grade Count:4
 120 - 265 MPa
@Temperature -40.0 - 80.0 °C
17400 - 38400 psi
@Temperature -40.0 - 176 °F
Average value: 193 MPa Grade Count:2
Poissons Ratio 0.330 - 0.4000.330 - 0.400Average value: 0.362 Grade Count:16
Shear Strength 90.0 - 105 MPa13100 - 15200 psiAverage value: 100 MPa Grade Count:3
Secant Modulus 5.00 - 18.0 GPa725 - 2610 ksiAverage value: 11.4 GPa Grade Count:4
 1.00 - 17.5 GPa
@Temperature 60.0 - 180 °C
145 - 2540 ksi
@Temperature 140 - 356 °F
Average value: 5.39 GPa Grade Count:3
 1.00 - 17.5 GPa
@Strain 0.000 - 15.0 %
145 - 2540 ksi
@Strain 0.000 - 15.0 %
Average value: 5.39 GPa Grade Count:3
Izod Impact, Notched 0.0600 - 6.51 J/cm0.112 - 12.2 ft-lb/inAverage value: 1.85 J/cm Grade Count:87
 1.10 - 7.36782 J/cm
@Temperature -40.0 - 149 °C
2.06 - 13.8029 ft-lb/in
@Temperature -40.0 - 300 °F
Average value: 3.97 J/cm Grade Count:2
Izod Impact, Unnotched 0.184 - 5340 J/cm0.345 - 10000 ft-lb/inAverage value: 14.0 J/cm Grade Count:27
Izod Impact, Notched (ISO) 6.00 - 54.0 kJ/m²2.86 - 25.7 ft-lb/in²Average value: 16.4 kJ/m² Grade Count:66
 11.0 - 111 kJ/m²
@Temperature -40.0 - -30.0 °C
5.23 - 52.8 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 16.9 kJ/m² Grade Count:30
Izod Impact, Unnotched (ISO) 75.0 - 103 kJ/m²35.7 - 49.0 ft-lb/in²Average value: 88.3 kJ/m² Grade Count:10
 80.0 - 96.0 kJ/m²
@Temperature -30.0 - -30.0 °C
38.1 - 45.7 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 88.0 kJ/m² Grade Count:7
Charpy Impact Unnotched 0.900 J/cm² - NB4.28 ft-lb/in² - NBAverage value: 9.23 J/cm² Grade Count:179
 0.900 J/cm² - NB
@Temperature -40.0 - -20.0 °C
4.28 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 8.55 J/cm² Grade Count:108
Charpy Impact, Notched 0.500 - 7.50 J/cm²2.38 - 35.7 ft-lb/in²Average value: 1.86 J/cm² Grade Count:196
 0.350 - 7.50 J/cm²
@Temperature -40.0 - -20.0 °C
1.67 - 35.7 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.58 J/cm² Grade Count:109
Dart Drop, Total Energy  9.99 - 23.5 J
@Temperature -20.0 - -20.0 °C
7.37 - 17.3 ft-lb
@Temperature -4.00 - -4.00 °F
Average value: 16.7 J Grade Count:1
 9.99 - 23.5 J
@Thickness 3.18 - 3.18 mm
7.37 - 17.3 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 16.7 J Grade Count:1
Puncture Energy 3.60 - 23.8 J2.66 - 17.6 ft-lbAverage value: 10.6 J Grade Count:4
 2.80 - 2.80 J
@Temperature -30.0 - -30.0 °C
2.07 - 2.07 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 2.80 J Grade Count:1
Tensile Creep Modulus, 1000 hours 5400 - 8000 MPa783000 - 1.16e+6 psiAverage value: 7470 MPa Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+17 ohm-cm1.00e+9 - 1.00e+17 ohm-cmAverage value: 2.32e+15 ohm-cm Grade Count:135
Surface Resistance 1.00e+10 - 1.50e+17 ohm1.00e+10 - 1.50e+17 ohmAverage value: 3.64e+15 ohm Grade Count:82
Dielectric Constant 3.30 - 14.03.30 - 14.0Average value: 4.80 Grade Count:35
Dielectric Strength 1.97 - 90.0 kV/mm50.0 - 2290 kV/inAverage value: 32.4 kV/mm Grade Count:108
Dissipation Factor 0.00900 - 0.3200.00900 - 0.320Average value: 0.0685 Grade Count:25
Arc Resistance 93.0 - 180 sec93.0 - 180 secAverage value: 132 sec Grade Count:12
Comparative Tracking Index 225 - 600 V225 - 600 VAverage value: 555 V Grade Count:85
Hot Wire Ignition, HWI 1.00 - 30.0 sec1.00 - 30.0 secAverage value: 15.1 sec Grade Count:11
High Amp Arc Ignition, HAI 1.00 - 120 arcs1.00 - 120 arcsAverage value: 112 arcs Grade Count:11
High Voltage Arc-Tracking Rate, HVTR 10.0 - 50.0 mm/min0.394 - 1.97 in/minAverage value: 19.9 mm/min Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 73.8 µm/m-°C2.78 - 41.0 µin/in-°FAverage value: 18.5 µm/m-°C Grade Count:78
 19.0 - 20.0 µm/m-°C
@Temperature 55.0 - 160 °C
10.6 - 11.1 µin/in-°F
@Temperature 131 - 320 °F
Average value: 14.1 µm/m-°C Grade Count:2
 11.0 - 19.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
6.11 - 10.6 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 14.1 µm/m-°C Grade Count:9
 11.0 - 19.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
6.11 - 10.6 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 14.1 µm/m-°C Grade Count:9
CTE, linear, Transverse to Flow 40.0 - 100 µm/m-°C22.2 - 55.6 µin/in-°FAverage value: 68.9 µm/m-°C Grade Count:56
 114 - 114 µm/m-°C
@Temperature 55.0 - 160 °C
63.3 - 63.3 µin/in-°F
@Temperature 131 - 320 °F
Average value: 114 µm/m-°C Grade Count:1
Specific Heat Capacity 1.30 - 1.50 J/g-°C0.311 - 0.359 BTU/lb-°FAverage value: 1.35 J/g-°C Grade Count:8
 1.87 - 1.87 J/g-°C
@Temperature 262 - 295 °C
0.447 - 0.447 BTU/lb-°F
@Temperature 504 - 563 °F
Average value: 1.87 J/g-°C Grade Count:2
Thermal Conductivity 0.330 - 0.533 W/m-K2.29 - 3.70 BTU-in/hr-ft²-°FAverage value: 0.396 W/m-K Grade Count:14
 0.310 - 0.310 W/m-K
@Temperature 262 - 295 °C
2.15 - 2.15 BTU-in/hr-ft²-°F
@Temperature 504 - 563 °F
Average value: 0.310 W/m-K Grade Count:2
Melting Point 220 - 325 °C428 - 617 °FAverage value: 262 °C Grade Count:189
Maximum Service Temperature, Air 100 - 270 °C212 - 518 °FAverage value: 174 °C Grade Count:59
Deflection Temperature at 0.46 MPa (66 psi) 215 - 266 °C419 - 510 °FAverage value: 255 °C Grade Count:108
Deflection Temperature at 1.8 MPa (264 psi) 208 - 285 °C406 - 545 °FAverage value: 251 °C Grade Count:230
Deflection Temperature at 8.0 MPa 165 - 249 °C329 - 480 °FAverage value: 199 °C Grade Count:37
Vicat Softening Point 200 - 260 °C392 - 500 °FAverage value: 247 °C Grade Count:45
Glass Transition Temp, Tg 20.0 - 70.0 °C68.0 - 158 °FAverage value: 47.9 °C Grade Count:4
Decomposition Temperature 310 °C590 °FAverage value: 310 °C Grade Count:6
UL RTI, Electrical 65.0 - 140 °C149 - 284 °FAverage value: 124 °C Grade Count:13
UL RTI, Mechanical with Impact 65.0 - 130 °C149 - 266 °FAverage value: 116 °C Grade Count:11
UL RTI, Mechanical without Impact 65.0 - 140 °C149 - 284 °FAverage value: 125 °C Grade Count:11
Flammability, UL94 HB - V-0HB - V-0Grade Count:147
Flame Spread 0.000 - 80.0 mm/min0.000 - 3.15 in/minAverage value: 8.50 mm/min Grade Count:12
Oxygen Index 23.0 - 32.0 %23.0 - 32.0 %Average value: 26.9 % Grade Count:17
Glow Wire Test 600 - 960 °C1110 - 1760 °FAverage value: 732 °C Grade Count:39
Ignition Temperature 350 - 400 °C662 - 752 °FAverage value: 383 °C Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 315 °C158 - 599 °FAverage value: 211 °C Grade Count:40
Nozzle Temperature 254 - 315 °C489 - 599 °FAverage value: 290 °C Grade Count:43
Die Temperature 300 - 320 °C572 - 608 °FAverage value: 311 °C Grade Count:8
Melt Temperature 143 - 340 °C290 - 644 °FAverage value: 290 °C Grade Count:154
Mold Temperature 26.7 - 160 °C80.0 - 320 °FAverage value: 88.5 °C Grade Count:159
Injection Velocity 50.8 - 80.0 mm/sec2.00 - 3.15 in/secAverage value: 69.0 mm/sec Grade Count:3
Drying Temperature 26.7 - 121 °C80.0 - 250 °FAverage value: 82.1 °C Grade Count:134
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.151 % Grade Count:76
Dew Point -30.0 - -17.8 °C-22.0 - 0.000 °FAverage value: -21.7 °C Grade Count:6
Injection Pressure 3.45 - 150 MPa500 - 21800 psiAverage value: 82.1 MPa Grade Count:31
Cushion 0.635 cm0.250 inAverage value: 0.635 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 60% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Glass Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 6, 50% Glass Fiber Filled

O2515 / 78014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.