  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Phenolic, Novolac, Flock Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Flock Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 - 1.45 g/cc0.0499 - 0.0524 lb/in³Average value: 1.41 g/cc Grade Count:7
Water Absorption 0.180 - 0.630 %0.180 - 0.630 %Average value: 0.436 % Grade Count:7
Linear Mold Shrinkage 0.00300 - 0.00850 cm/cm0.00300 - 0.00850 in/inAverage value: 0.00576 cm/cm Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 63.0 - 91.063.0 - 91.0Average value: 77.7 Grade Count:7
Tensile Strength, Ultimate 36.0 - 55.7 MPa5220 - 8080 psiAverage value: 48.6 MPa Grade Count:7
Elongation at Break 0.710 - 1.00 %0.710 - 1.00 %Average value: 0.817 % Grade Count:6
Modulus of Elasticity 6.90 - 8.27 GPa1000 - 1200 ksiAverage value: 7.70 GPa Grade Count:6
Flexural Yield Strength 61.0 - 83.2 MPa8850 - 12100 psiAverage value: 74.2 MPa Grade Count:7
Flexural Modulus 6.20 - 7.72 GPa899 - 1120 ksiAverage value: 7.12 GPa Grade Count:7
Compressive Yield Strength 139 - 213 MPa20200 - 30900 psiAverage value: 175 MPa Grade Count:7
Poissons Ratio 0.300 - 0.3500.300 - 0.350Average value: 0.338 Grade Count:4
Shear Modulus 2.56 - 3.00 GPa371 - 435 ksiAverage value: 2.87 GPa Grade Count:4
Izod Impact, Notched 0.210 - 0.277 J/cm0.393 - 0.519 ft-lb/inAverage value: 0.241 J/cm Grade Count:6
Charpy Impact, Notched 0.199 - 0.400 J/cm²0.947 - 1.90 ft-lb/in²Average value: 0.271 J/cm² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 6.38e+10 - 2.13e+12 ohm-cm6.38e+10 - 2.13e+12 ohm-cmAverage value: 5.65e+11 ohm-cm Grade Count:7
Dielectric Constant 4.50 - 6.604.50 - 6.60Average value: 5.14 Grade Count:7
Dielectric Strength 7.90 - 16.2 kV/mm201 - 411 kV/inAverage value: 11.1 kV/mm Grade Count:7
Dissipation Factor 0.0400 - 0.07600.0400 - 0.0760Average value: 0.0560 Grade Count:7
Arc Resistance 26.0 - 160 sec26.0 - 160 secAverage value: 110 sec Grade Count:7
Comparative Tracking Index 150 - 175 V150 - 175 VAverage value: 168 V Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 44.0 - 67.0 µm/m-°C
@Temperature 40.0 - 130 °C
24.4 - 37.2 µin/in-°F
@Temperature 104 - 266 °F
Average value: 54.0 µm/m-°C Grade Count:3
Thermal Conductivity 0.370 - 0.400 W/m-K
@Temperature 100 - 100 °C
2.57 - 2.78 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.385 W/m-K Grade Count:2
Maximum Service Temperature, Air 170 - 200 °C338 - 392 °FAverage value: 189 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 156 - 196 °C313 - 385 °FAverage value: 173 °C Grade Count:7
Flammability, UL94 HB - V-0HB - V-0Grade Count:7
Oxygen Index 24.2 - 27.1 %24.2 - 27.1 %Average value: 25.7 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PEN-PET
Overview of materials for PEKK, Unreinforced
Overview of materials for PEKK, Reinforced
Overview of materials for PCTG Copolyester
Overview of materials for PCTA Polyester Alloy

O2719 / 78089

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.