MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toyobo Zenite® 650 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Product Description: Zenite 650 is designed for high dielectric constant and low dissipation factor

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.02 g/cc0.0730 lb/in³ISO 1183
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 143 MPa20700 psiISO 527-2/50
Elongation at Break 1.5 %1.5 %ISO 527-2/50
Tensile Modulus 18.0 GPa2610 ksiISO 527-1
Flexural Strength 197 MPa28600 psiISO 178
Flexural Modulus 16.0 GPa2320 ksiISO 178
Charpy Impact Unnotched 2.31 J/cm²11.0 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 12
@Frequency 2.00e+9 Hz
12
@Frequency 2.00e+9 Hz
IEC 61189-2-721
Dielectric Strength 24.0 kV/mm610 kV/inAC; IEC 60243-1
Dissipation Factor 0.0080
@Frequency 2.00e+9 Hz
0.0080
@Frequency 2.00e+9 Hz
IEC 61189-2-721
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 278 °C532 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 295 °C563 °F
Middle Barrel Temperature 315 °C599 °F
Front Barrel Temperature 335 °C635 °F
Nozzle Temperature 335 °C635 °F
Zone 4 335 °C635 °FInjection
Melt Temperature 340 °C644 °F
Mold Temperature 100 °C212 °F
Drying Temperature 150 °C302 °F
Dry Time 6.00 hour6.00 hour
Injection Pressure 75.2 MPa10900 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6330 / 311023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.