MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo CoolPoly® E5521 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Product Description: CoolPoly E series of thermally conductive plastics transfers heat, is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Use: Automotive Applications

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³ISO 1183
Maximum Moisture Content 0.0100.010
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 32.0 MPa4640 psiISO 527-2/5
Elongation at Break 0.70 %0.70 %ISO 527-2/5
Tensile Modulus 7.10 GPa1030 ksiISO 527-1
Flexural Strength 56.0 MPa8120 psiISO 178
Flexural Modulus 11.1 GPa1610 ksiISO 178
Charpy Impact Unnotched 0.336 J/cm²1.60 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.252 J/cm²1.20 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness 66 dB
@Frequency 1e+9 Hz
66 dB
@Frequency 1e+9 Hz
EMI; ASTM D4935
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 4.47 W/m-K31.0 BTU-in/hr-ft²-°FThruplane; ASTM D1461
 34.6 W/m-K240 BTU-in/hr-ft²-°FFlow; ASTM D1461
Deflection Temperature at 1.8 MPa (264 psi) 198 °C388 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 332 - 360 °C630 - 680 °F
Middle Barrel Temperature 338 - 371 °C640 - 700 °F
Front Barrel Temperature 343 - 382 °C649 - 720 °F
Nozzle Temperature 349 - 382 °C660 - 720 °F
Mold Temperature 92.8 - 177 °C199 - 351 °F
Drying Temperature 180 °C356 °F
Dry Time 4.00 hour4.00 hour
Back Pressure <= 0.350 MPa<= 50.8 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6275 / 310968

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.