MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: 30% glass fiber, low melt flow for extrusion and injection molding

AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin retains most of the desirable ultra-performance attributes of glass reinforced PEEK, including chemical resistance, fatigue resistance and long term thermal oxidative stability, but the heat deflection temperature is lower than 30% GF PEEK.

The material's excellent balance of properties makes it well suited for demanding applications across a broad range of industries including healthcare, transportation, electronics, oil and gas, and chemical processing.

- Beige: AV-621 GF30 BG 20
- Black: AV-621 GF30 BK 95

Markets/Uses: Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Compressor Components

Applications: Industrial Applications; Medical Devices; Medical/Healthcare Applications

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Injection notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Viscosity 650 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
650 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm
@Thickness 3.18 mm
0.0090 - 0.011 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 101101ASTM D785
Tensile Strength 147 MPa21300 psi5.0 mm/min; ASTM D638
Tensile Strength, Yield 158 MPa22900 psiType 1A, 5 mm/min; ISO 527-2
Elongation at Break 3.2 %3.2 %5.0 mm/min; ASTM D638
 3.2 %3.2 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 9.90 GPa1440 ksi5.0 mm/min; ASTM D638
 10.6 GPa1540 ksi1 mm/min, Type 1A; ISO 527-2
Flexural Strength 236 MPa34200 psiISO 178
 237 MPa34400 psiASTM D790
Flexural Modulus 9.40 GPa1360 ksiASTM D790
 9.80 GPa1420 ksiISO 178
Compressive Strength 159 MPa23100 psiASTM D695
Poissons Ratio 0.430.43ASTM E132
Shear Strength 84.5 MPa12300 psiASTM D732
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inASTM D256
Izod Impact, Unnotched 10.0 J/cm18.7 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 70.0 kJ/m²33.3 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+17 ohm-cm2.10e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohm>= 1.90e+17 ohmASTM D257
Dielectric Constant  3.48
@Frequency 1e+6 Hz
3.48
@Frequency 1e+6 Hz
ASTM D150
 3.52
@Frequency 60 Hz
3.52
@Frequency 60 Hz
ASTM D150
 3.53
@Frequency 1000 Hz
3.53
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.00 mm
381 kV/in
@Thickness 0.118 in
ASTM D149
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
9.44 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
Specific Heat Capacity  1.29 J/g-°C
@Temperature 50.0 °C
0.308 BTU/lb-°F
@Temperature 122 °F
ASTM C351
 1.66 J/g-°C
@Temperature 200 °C
0.397 BTU/lb-°F
@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FASTM C177
Melting Point 340 °C644 °FPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 217 °C423 °FAnnealed; ASTM D648
Glass Transition Temp, Tg 158 °C316 °FDSC
Flammability, UL94  V-1
@Thickness 0.800 mm
V-1
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 366 °C691 °F
Middle Barrel Temperature 371 °C700 °F
Front Barrel Temperature 377 °C711 °F
Nozzle Temperature 382 °C720 °F
Melt Temperature 366 - 388 °C691 - 730 °FInjection
Mold Temperature 149 - 177 °C300 - 351 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBeige; Black
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4148 / 279948

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.