MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemical Concepts PERMATEX® #66 Clear Silicone Adhesive Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Permatex® Clear Silicone Adhesive Sealant is a general purpose, single component, room temperature vulcanizing (RTV) adhesive/sealant compound, designed for the sealing of mechanical assemblies. Upon curing from the exposure to moisture in the air, this non-sagging paste forms a tough, flexible, waterproof seal of silicone rubber, which resists aging, weathering and thermal cycling without hardening, shrinking or cracking. Conforms to MIL-A-46106B, Type I. Permatex® Clear RTV Silicone Adhesive Sealant shall meet the requirements of the FDA ‘Code of Federal Regulations 21CFR’ concerning food contact applications if used in accordance with its Section 177.2600: ‘Rubber Articles Intended for Repeated Use’.

Features:

  • Easy application• Applied to horizontal or vertical surfaces
  • Superior adhesion and flexibility
  • Waterproofs
  • Insulates
  • Unaffected by vibration
  • Non-flammable
  • Non-toxic
Permatex® Clear Silicone Adhesive Sealant is an excellent allpurpose adhesive/sealant for the following materials;
  • Metal
  • Glass
  • Wood
  • Plastic
  • Vulcanized silicone rubber
  • Ceramics
  • Natural and synthetic fibers
  • Painted surfaces.

Cures on exposure to moisture in the air. The product cures tack free in 1 hour and fully cures in 24 hours, depending on temperature, humidity and gap.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 20
@Temperature 25.0 °C
>= 20
@Temperature 77.0 °F
Cured after 7 days, 50% RH
Tensile Strength >= 1.50 MPa>= 218 psiCured after 7 days, 50% RH, @ 25°C
Elongation at Break >= 350 %>= 350 %Cured after 7 days, 50% RH
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Extrusion Rate >= 220 g/min
@Temperature 25.0 °C
>= 220 g/min
@Temperature 77.0 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Appearancenon sag paste
Chemical CompositionAcetoxy Silicone Rubber
Colorclear
Temperature Resistance-75 to 40°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI982 / 232175

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.